Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Delrin® FG511DP NC010 - POM - DuPont Engineering Polymers

Material Data Center offers the following functions for Delrin® FG511DP NC010:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Delrin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
Common features of Delrin® acetal resins include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents, and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating, and available in a variety of colors and speciality grades.

Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics, and consumer goods industries.

Delrin® FG511DP is a medium viscosity acetal homopolymer with enhanced crystallization for faster cycle times and excellent creep and fatigue resistance. It has improved thermal stability, excellent dimensional stability, low warpage and fewer voids. It has been developed for applications in contact with food.

FOOD CONTACT
This product is manufactured according to Good Manufacturing Practice (GMP) principles and generally accepted in food contact applications in Europe and the USA when meeting applicable use conditions. For details, individual compliance statements are available from your DuPont representative. 
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 13 cm³/10min ISO 1133
Temperatura 190 °C -
Carga 2.16 kg -
Contração após a moldagem, paralelo 1.9 % ISO 294-4, 2577
Contração após a moldagem, perpendicular 1.8 % ISO 294-4, 2577
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 3500 MPa ISO 527
Tensão no escoamento 75 MPa ISO 527
Deformação no escoamento 12 % ISO 527
Deformação nominal na ruptura 25 % ISO 527
Resistência ao impacto Charpy , +23°C 220 kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C 200 kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 6.5 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 6 kJ/m² ISO 179/1eA
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 178 °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 107 °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 163 °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 160 °C ISO 306
Coef. de expansão térmica linear, paralelo 100 E-6/K ISO 11359-1/-2
Coef. de expansão térmica linear, perpend. 110 E-6/K ISO 11359-1/-2
Outras propriedadesValorUnidadeMétodo de ensaio
Absorção de água 0.9 % Sim. to ISO 62
Absorção de umidade 0.3 % Sim. to ISO 62
Densidade 1420 kg/m³ ISO 1183
Diagrama
Tensão - deformação , Delrin® FG511DP NC010, POM, DuPont
Módulo secante - deformação , Delrin® FG511DP NC010, POM, DuPont
Características
Processamento
Moldagem por injeção, Extrusão de perfis, Extrusão de chapas, Outros tipos de extrusão
Forma de entrega
Granulos, Cor natural
Aditivos
Lubrificantes, Desmoldante
Características
Homopolímero
Disponibilidade regional
Outras informações
Moldagem por injeção
Drying is recommended, but not necessary for newly opened packaging stored in a dry location.
Follow the drying guidelines above in the following cases:

·         If moisture is above the Processing Moisture Content recommendation,

·         When a resin container is damaged,

·         When the material is not properly stored in a dry place at room temperature, or

·         When packaging stays open for a significant time.

Resistência em meio químico
Ácidos
Ácido Acético (5% em massa) (23°C)
Solução de Ácido Cítrico (10% em massa) (23°C)
Ácido Láctico (10% em massa) (23°C)
Ácido Hidroclorídrico (36% em massa) (23°C)
Ácido Nítrico (40% em massa) (23°C)
Ácido Sulfúrico (38% em massa) (23°C)
Ácido Sulfúrico (5% em massa) (23°C)
Solução de Ácido Crômico (40% em massa) (23°C)
Bases
Solução de Hidróxido de Sódio (35% em massa) (23°C)
Solução de Hidróxido de Sódio (1% em massa) (23°C)
Solução de Hidróxido de Amônio (10% em massa) (23°C)
Álcoois
Álcool isopropílico (23°C)
Metanol (23°C)
Etanol (23°C)
Hidrocarbonetos
n-Hexano (23°C)
Tolueno (23°C)
Iso-Octano (23°C)
Cetonas
Acetona (23°C)
Éteres
Di-etil éter (23°C)
Óleos Minerais
Óleo de motor multissérie SAE 10W40 (23°C)
Óleo de motor multissérie SAE 10W40 (130°C)
Óleo de engrenagem hipóide SAE 80/90 (130°C)
Óleo isolante (23°C)
Combustíveis Padrões
Líquido 1 ISO 1817 (60°C)
Líquido 2 ISO 1817 (60°C)
Líquido 3 ISO 1817 (60°C)
Líquido 4 ISO 1817 (60°C)
Combustível padrão sem álcool (pref. Líquico C ISO 1817) (23°C)
Combustível padrão com álcool (pref. Líquico 4 ISO 1817) (23°C)
Diesel (pref. Líquido F ISO 1817) (23°C)
Diesel (pref. Líquido F ISO 1817) (90°C)
Diesel (pref. Líquido F ISO 1817) (>90°C)
Soluções de sais
Solução de Cloreto de Sódio (10% em massa) (23°C)
Solução de Hipoclorito de Sódio (10% em massa) (23°C)
Solução de Carbonato de Sódio (20% em massa) (23°C)
Solução de Carbonato de Sódio (2% em massa) (23°C)
Solução de Cloreto de Zinco (50% em massa) (23°C)
Outras
Acetato de Etila (23°C)
Peróxido de Hidrogênio (23°C)
Fluido de freio DOT No. 4 (130°C)
Etileno Glicol (50% em massa) em água (108°C)
1% de Etanol (nonilfenoxi-polioxietileno) em água (23°C)
(50% Ácido Oleico + 50% Azeite de Oliva) (23°C)
Água (23°C)
Água Deionizada (90°C)
Solução Fenólica (5% em massa) (23°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.