Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of AKROLEN® PP GFM 25/15 black (1415) - PP-(GF+MX)40 - Akro-Plastic GmbH

Material Data Center offers the following functions for AKROLEN® PP GFM 25/15 black (1415):
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Akrolen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 13.5 cm³/10min ISO 1133
Temperatura 230 °C -
Carga 2.16 kg -
Contração após a moldagem, paralelo 0.5 % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.8 % ISO 294-4, 2577
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 6500 MPa ISO 527
Tensão na ruptura 75 MPa ISO 527
Deformação na ruptura 75 % ISO 527
Módulo de flexão, 23°C 6600 MPa ISO 178
Resistência à flexão 105 MPa ISO 178
Resistência ao impacto Charpy, +23°C 45 kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C 45 kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 10 kJ/m² ISO 179/1eA
Impacto Izod com entalhe, +23°C 10 kJ/m² ISO 180/1A
Ball indentation hardness 100 MPa ISO 2039-1
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 167 °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 150 °C ISO 75-1/-2
Temperatura de deflexão térmica , 0.45 MPa 163 °C ISO 75-1/-2
Coef. de expansão térmica linear, paralelo 20 E-6/K ISO 11359-1/-2
Coef. de expansão térmica linear, perpend. 125 E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. HB class IEC 60695-11-10
Espessuras do tubo de teste 1.6 mm -
Propriedades elétricasValorUnidadeMétodo de ensaio
ISO Dados
Resistividade volumétrica específica 2E9 Ohm*m IEC 62631-3-1
Resistência elétrica 18 kV/mm IEC 60243-1
Índice comparativo de linha de fuga 600 - IEC 60112
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1210 kg/m³ ISO 1183
Diagrama
Viscosidade - taxa de cisalhamento , AKROLEN® PP GFM 25/15 black (1415), PP-(GF+MX)40, Akro-Plastic
Tensão de cisalhamento - taxa de cisalhamento , AKROLEN® PP GFM 25/15 black (1415), PP-(GF+MX)40, Akro-Plastic
Volume específico - temperatura (pvT) , AKROLEN® PP GFM 25/15 black (1415), PP-(GF+MX)40, Akro-Plastic
Características
Forma de entrega
Negro
Características especiais
Estável contra o calor
Aplicaciones
Automóvel, Elétrica e Eletrônica
Disponibilidade regional
Europa, Ásia Pacífico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.