Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of SABIC® HDPE M864SE - (PE-HD) - Saudi Basic Industries Corporation (SABIC)
Material Data Center offers the following functions for SABIC® HDPE M864SE:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
제품 설명서
SABIC® HDPE M864SE is an UV stabilized, high density polyethylene injection molding grade with a narrow molecular weight distribution. It is typically used for injection molding applications where rigidity, toughness and warp resistance are required.
SABIC® HDPE M864SE is typically used for the manufacture of injection molded cases, crates, trays, industrial pails and other similar items.
Processing conditions.
Typical molding conditions for SABIC® HDPE M864SE are: Melt temperature: 230 - 275 °C (450 - 525 °F); Mold temperature: 32 - 38 °C (90 - 100 °F); Injection pressure: 69 - 89 MPa (10000 - 13000 PSI)
This product is not intended for and must not be used in any pharmaceutical/medical applications.
기계적 특성 | 값 | 단위 | 시험규격 |
ISO 데이터 |
인장탄성률 |
1450 |
MPa |
ISO 527 |
항복강도 |
32 |
MPa |
ISO 527 |
파단시 강도 |
15 |
MPa |
ISO 527 |
파단시 신율 |
>50 |
% |
ISO 527 |
굴곡 계수, 23°C |
1700 |
MPa |
ISO 178 |
굴곡 강도 |
32 |
MPa |
ISO 178 |
쇼어 D 경도 |
65 |
- |
ISO 7619-1 |
열적 특성 | 값 | 단위 | 시험규격 |
ISO 데이터 |
녹는점, 10°C/min |
135 |
°C |
ISO 11357-1/-3 |
하중하에서의 변형온도, 0.45 MPa |
95 |
°C |
ISO 75-1/-2 |
비카트 연화 온도, A |
129 |
°C |
ISO 306 |
특징
생산 공정
사출 성형
특별 특성
U.V. 안정성 또는 기후 안정성
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.