Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® HDPE F00950 - (PE-HD) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® HDPE F00950:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
SABIC® HDPE F00950 resin is a high molecular weight, high density polyethylene copolymer. The design of the product, molecular architecture and density, gives F00950 a good balance of easy extrusion and high melt strength with strong physical properties. SABIC® HDPE F00950 is typically used for production of thin films with good strength and rigidity. The material contains anti-oxidants. SABIC® HDPE F00950 resin is typically used for blown film extrusion and production of high strength grocery sacks, shopping bags and high quality thin films for multi wall sack liners and replacement for thin paper products. SABIC® HDPE F00950 can be extruded on conventional HMW-HDPE equipment with temperature settings between 200 and 220°C. Film properties have been measured at 25 µm films with a BUR = 4.Film has been produced on Kiefel IBC film blown line at 160 kg/h with a die of 150 mm, die gap of 1.2 mm and a frostline height of 150 cm (= 10D). This product is not intended for and must not be used in any pharmaceutical/medical applications.
기계적 성질 (필름) 단위시험규격
ISO 데이터
인장탄성률, 평행 620 MPa ISO 527-3
인장탄성률, 수직 620 MPa ISO 527-3
항복시의 강도, 평행 30 MPa ISO 527-3
항복시의 강도, normal 30 MPa ISO 527-3
파단시 강도, 평행 40 MPa ISO 527-3
파단시 강도, 수직 50 MPa ISO 527-3
트라우저 전단강도, 평행 6 N/mm ISO 6383-1
트라우저 전단강도, 수직 20 N/mm ISO 6383-1
특징
특성
Copolymer
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.