Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL™ Resin PX138H - Asia - (PPE+PS)-GF20 - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL™ Resin PX138H - Asia:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
NORYL™ PX138H resin is a 20% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade exhibits very low moisture absorption, high strength, hydrolytic stability, Low warpage, low specific gravity, and dimensional stability.

UL Yellow Card Link E207780-228575
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 2 cm³/10min ISO 1133
온도 280 °C -
하중 5 kg -
ASTM 데이터
용융 흐름성, MFI 2.7 g/10min ASTM D 1238
온도 280 °C -
하중 5 kg -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 6000 MPa ISO 527
항복강도 90 MPa ISO 527
항복변형률 3 % ISO 527
파단시 강도 90 MPa ISO 527
파단시 신율 3 % ISO 527
굴곡 계수 5400 MPa ISO 178
챠피 노치드 충격 강도, +23°C 8 kJ/m² ISO 179/1eA
아이조드 노치 충격 강도, +23°C, 4mm 30 kJ/m² ISO 180/1A
아이조드 노치 충격 강도, -30°C, 4mm 33 kJ/m² ISO 180/1A
ASTM 데이터
인장탄성률 6500 MPa ASTM D 638
항복강도 100 MPa ASTM D 638
파단시 강도 100 MPa ASTM D 638
항복변형률 3 % ASTM D 638
파단시 신율 3 % ASTM D 638
굴곡 계수 5300 MPa ASTM D 790
아이조드 충격은 노치, 1/8 in 90 J/m ASTM D 256
아이조드 충격은 노치, Low-Temperature 100 J/m ASTM D 256
온도 -30 °C -
열적 특성단위시험규격
ISO 데이터
하중하에서의 변형온도, 1.80 MPa 135 °C ISO 75-1/-2
비카트 연화 온도, B 143 °C ISO 306
비카트 연화 온도, 120°C/h 50N 147 °C ISO 306
1.5mm 평균두께에서의 난연성 HB class IEC 60695-11-10
테스트 두께 1.5 mm -
ASTM 데이터
DTUL @ 264 psi 137 °C ASTM D 648
비카트 연화 온도 143 °C ASTM D 1525
기타 특성단위시험규격
물에서의 흡수성 0.12 % ISO 62와 유사
조건에서의 흡습성 0.04 % ISO 62와 유사
밀도 1230 kg/m³ ISO 1183
밀도 1230 kg/m³ ASTM D 792
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 110 - 120 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.02 % -
용융수지온도 300 - 325 °C -
성형온도 80 - 110 °C -
Zone 1 265 - 315 °C -
Zone 2 275 - 320 °C -
Zone 3 290 - 325 °C -
Screw speed 20 - 100 rpm -
Back pressure 0.3 - 0.7 MPa -
특징
생산 공정
사출 성형
내화학성에
Hydrolytically Stable
지역별 검색
쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.