Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL™ Resin GFN1F - Americas - (PPE+PS)-GF10 - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL™ Resin GFN1F - Americas:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
NORYL™ GFN1F resin is a 10% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade exhibits very low moisture absorption, high strength, hydrolytic stability, Low warpage, low specific gravity, and dimensional stability. NORYL GFN1F carries a UL746C outdoor suitability rating of F1 along with FDA food contact compliance and NSF 61 listings in several colors. The properties of this material makes it an excellent candidate for water management applications such as water filter and meter components, pump housings / impellers, shower + faucet, and valves.*See NORYL GFN1 resin for NON FDA / NSF version.

UL Yellow Card Link E121562-221234
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 16 cm³/10min ISO 1133
온도 300 °C -
하중 5 kg -
ASTM 데이터
용융 흐름성, MFI 16.6 g/10min ASTM D 1238
온도 300 °C -
하중 5 kg -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 4400 MPa ISO 527
파단시 강도 64 MPa ISO 527
파단시 신율 3 % ISO 527
굴곡 계수 4160 MPa ISO 178
굴곡 강도 122 MPa ISO 178
챠피 충격 강도, +23°C 34 kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C 33 kJ/m² ISO 179/1eU
Izod impact strength, +23°C, 4mm 27 kJ/m² ISO 180/1U
Izod impact strength, -30°C, 4mm 25 kJ/m² ISO 180/1U
아이조드 노치 충격 강도, +23°C, 4mm 10 kJ/m² ISO 180/1A
아이조드 노치 충격 강도, -30°C, 4mm 9 kJ/m² ISO 180/1A
ASTM 데이터
인장탄성률 4350 MPa ASTM D 638
파단시 강도 63 MPa ASTM D 638
파단시 신율 3 % ASTM D 638
굴곡 계수 3840 MPa ASTM D 790
로크웰 경도 L104 - ASTM D 785
아이조드 충격은 노치, 1/8 in 118 J/m ASTM D 256
아이조드 충격은 노치, Low-Temperature 103 J/m ASTM D 256
온도 -30 °C -
Izod충격강도, 1/8 in 449 J/m ASTM D 256
열적 특성단위시험규격
ISO 데이터
비카트 연화 온도, B 131 °C ISO 306
비카트 연화 온도, 120°C/h 50N 134 °C ISO 306
1.5mm 평균두께에서의 난연성 HB class IEC 60695-11-10
테스트 두께 1.5 mm -
ASTM 데이터
DTUL @ 66 psi 131 °C ASTM D 648
DTUL @ 264 psi 122 °C ASTM D 648
전기적 특성단위시험규격
ASTM 데이터
소산 인자, 1 MHz 0.0014 - ASTM D 150
상대 유전율, 1 MHz 2.9 - ASTM D 150
기타 특성단위시험규격
밀도 1130 kg/m³ ASTM D 792
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 105 - 110 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.02 % -
용융수지온도 295 - 315 °C -
성형온도 75 - 105 °C -
Zone 1 260 - 305 °C -
Zone 2 270 - 310 °C -
Zone 3 280 - 315 °C -
Screw speed 20 - 100 rpm -
Back pressure 0.3 - 0.7 MPa -
특징
생산 공정
사출 성형
내화학성에
Hydrolytically Stable
Certifications
Food contact, Food approval FDA 21 CFR
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.