Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEXAN™ Copolymer EXL1414 - Asia - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for LEXAN™ Copolymer EXL1414 - Asia:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lexan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
LEXAN EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excellent processability and release with opportunities for shorter IM cycle times compared to standard PC. LEXAN EXL1414 resin is a product available in wide range of opaque colors and may be an excellent candidate for a wide variety of applications.

UL Yellow Card Link E207780-228376
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 9 cm³/10min ISO 1133
온도 300 °C -
하중 1.2 kg -
ASTM 데이터
용융 흐름성, MFI 10 g/10min ASTM D 1238
온도 300 °C -
하중 1.2 kg -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 2150 MPa ISO 527
항복강도 57 MPa ISO 527
항복변형률 6 % ISO 527
파단시 강도 60 MPa ISO 527
파단시 신율 50 % ISO 527
굴곡 계수 2250 MPa ISO 178
챠피 충격 강도, +23°C, 3mm N kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C, 3mm N kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C, 3mm 70 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C, 3mm 65 kJ/m² ISO 179/1eA
Izod충격강도, +23°C N kJ/m² ISO 180/1U
아이조드 노치 충격 강도, +23°C, 3mm 70 kJ/m² ISO 180/1A
아이조드 노치 충격 강도, -30°C, 3mm 60 kJ/m² ISO 180/1A
ASTM 데이터
인장탄성률 2020 MPa ASTM D 638
항복강도 55 MPa ASTM D 638
파단시 강도 50 MPa ASTM D 638
항복변형률 6 % ASTM D 638
파단시 신율 98 % ASTM D 638
굴곡 계수 2230 MPa ASTM D 790
로크웰 경도 R 121 - ASTM D 785
아이조드 충격은 노치, 1/8 in 865 J/m ASTM D 256
아이조드 충격은 노치, Low-Temperature 774 J/m ASTM D 256
온도 -30 °C -
열적 특성단위시험규격
ISO 데이터
비카트 연화 온도, B 145 °C ISO 306
비카트 연화 온도, 120°C/h 50N 146 °C ISO 306
두께 H인 제품의 난연성 HB class IEC 60695-11-10
테스트 두께 0.4 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM 데이터
DTUL @ 66 psi 139 °C ASTM D 648
DTUL @ 264 psi 124 °C ASTM D 648
비카트 연화 온도 145 °C ASTM D 1525
전기적 특성단위시험규격
ASTM 데이터
전기 압력, 단기간의 16.2 kV/mm ASTM D 149
소산 인자, 1 MHz 0.0093 - ASTM D 150
상대 유전율, 1 MHz 2.64 - ASTM D 150
표면 저항 1E15 Ohm ASTM D 257
부피 저항 1E15 Ohm*cm ASTM D 257
기타 특성단위시험규격
물에서의 흡수성 0.35 % ISO 62와 유사
조건에서의 흡습성 0.15 % ISO 62와 유사
밀도 1190 kg/m³ ISO 1183
밀도 1180 kg/m³ ASTM D 792
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 120 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.02 % -
용융수지온도 295 - 315 °C -
성형온도 70 - 95 °C -
Zone 1 270 - 295 °C -
Zone 2 280 - 305 °C -
Zone 3 295 - 315 °C -
Screw speed 40 - 70 rpm -
Back pressure 0.3 - 0.7 MPa -
특징
생산 공정
사출 성형
응용
자동차의
지역별 검색
쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.