Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kepstan® 8010G30 - PAEK-GF30 - ARKEMA

Material Data Center offers the following functions for Kepstan® 8010G30:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kepstan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서

KEPSTAN® PEKK resin is a high performance thermoplastic material, based on PolyEtherKetoneKetone (PEKK) highly stable chemical backbone. KEPSTAN® is a unique member of the PAEK family that incorporates distinctive structural features that allow for exceptional possibilities in the control of crystallinity. These features include a low Ether/Ketone ratio and a copolymer structure incorporating Terephthalic and Isophthalic moieties. 


KEPSTAN® 8010G30 resin is a glass fiber reinforced compound, based on the 8000 series of KEPSTAN® resins. This series offers the highest glass transition temperature and the highest crystallinity, leading to the best tensile and compression strengths among the different series of KEPSTAN® PEKK copolymers.


KEPSTAN® 8010G30 resin is a low flow grade, suitable for extrusion, compression and injection molding. 


KEPSTAN® 8010G30 resin is available in pellet form and standard packaging is 10 kg boxes.

Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 7 cm³/10min ISO 1133
온도 380 °C -
하중 5 kg -
기타 특성단위시험규격
밀도 1520 kg/m³ ISO 1183
기타 정보
사E성
Drying temperature and time: 150°C for 3 to 4 hours or 120°C for 6 to 8 hours
Processing temperature: 375 – 385°C
Temperature settings - Injection: Rear 350°C / Center 375°C / Front 375°C / Nozzle 385°C
Mold temperature (to facilitate filling of the cavity and polymer crystallization): 230 - 240°C
Temperature settings - Extrusion:  Zones 1/2/3/4: 355°C/ 370°C/ 385°C/ 385°C   Die: 370°C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.