Material datasheets available free. Online registration at: www.materialdatacenter.com
Epikote - EP - Hexion
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Epikote" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
... in toughness improvement. Practical Example A practical example will serve to illustrate this: Blends with different contents of core-shell particles were produced from an aromatic bisphenol A epoxy resin (grade: Epikote 828, manufacturer: Resolution) and cured at 120 to 180°C with diaminodiphenyl sulfone (DDS) in the form of 4mm-thick sheets. The problem frequently encountered in incorporating nanoscale particles into reactive resins is agglomeration. This results in undesirable rheological ...
Kunststoffe international, 2012-06-25, CRP Components with Class A Surfaces
...w glass transition temperature. Investigations conducted on the various resin systems revealed significant differences in the course of specific volume changes subject to temperature. The least shrinkage was found in the resin system (grade: Epikote 04695/1, manufacturer: Momentive Specialty Chemicals GmbH, Duisburg, Germany). Design and Construction of a High-pressure Gap Impregnation Plant In order to examine more closely the factors influencing the surface qualities of FRP components, the IKV...
Kunststoffe international, 2014-10-10, Resins and Reactive Systems
...e trays, bumpers and crash boxes can be produced more than 100,000 times every year. The various raw material suppliers recently adapted their basic thermolatent special types of epoxy resins, i. e. the brands of Baxxodur, Voraforce, Epikote and Araldite, to fit fast curing [12–15]. Viscosities are below 200 mPas, which is a value extraordinarily low. This makes it possible to soak the semi-finished fiber product within a period clearly below one minute, subject to the respective component; cur...
Kunststoffe international, 2015-08-17, Additive Preforming for High-Volume Production
...& Co. KG, Rietberg, GermanyMaterial:Glass fiberGlass fiber coated with polyester und copolyamideType:R63SX3Kuper Commingled YarnLinear density:4,800 tex42 texRTM-processResin systemSupplier:Momentive Specialty Chemicals GmbH, Duisburg, GermanyResin:Epikote resin 05475Hardener:Epikure curing agent 05443Curing temperature:15 min at 80 °CSupplierMaterialAreal weightLayerLayupCalculated FVCSaertex GmbH & Co. KG, Saerbeck, GermanySaertex UD-NCF248 g/m²12[0° /90° /0°]438.9 %Owens Corning Inc., Toledo...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.