Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Grilamid TR 90 UV LS natural - PAMACM12 - EMS-GRIVORY | a unit of EMS-CHEMIE AG

Material Data Center offers the following functions for Grilamid TR 90 UV LS natural:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Grilamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Product-nomenclature: ISO 16396-PAMACM12,,GTL1,C14-020

 

Product Attributes

  Highly transparent, Improved UV resistance (outdoor use)

Markets

  Automotive
  Automotive electr. and electronics, lighting, Cooling and climate control, Fuel systems,
Powertrain and Chassis, Interior, Exterior
  Electricals & Electronics
  Electrical equipment, Lighting
  Industry & Consumer goods
  Hydraulics & Pneumatics, Mechanical Engineering, Sports & Leisure, Tools & Accessories

Approvals

  Food Contact
  EU Requirements, FDA
Processing/Physical Characteristics乾燥/調湿単位テスト基準
ISO データ
成形収縮率, 平行 0.7 / * % ISO 294-4, 2577
成形収縮率, 直角 0.8 / * % ISO 294-4, 2577
機械的特性乾燥/調湿単位テスト基準
ISO データ
引張弾性率 1600 / 1600 MPa ISO 527
降伏応力 60 / 60 MPa ISO 527
降伏ひずみ 8 / 6 % ISO 527
破壊呼びひずみ >50 / >50 % ISO 527
シャルピー衝撃強さ, +23°C N / N kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C N / N kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 13 / 13 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 12 / 12 kJ/m² ISO 179/1eA
ショア硬さD 81 / * - ISO 7619-1
熱的特性乾燥/調湿単位テスト基準
ISO データ
ガラス転移点, 10°C/min 155 / * °C ISO 11357-1/-2
荷重たわみ温度, 1.80 MPa 115 / * °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 135 / * °C ISO 75-1/-2
線膨張係数, 平行 90 / * E-6/K ISO 11359-1/-2
線膨張係数, 直角 90 / * E-6/K ISO 11359-1/-2
厚さhでの燃焼性 HB / * class IEC 60695-11-10
試験片の厚さ 0.8 / * mm -
電気的特性.乾燥/調湿単位テスト基準
ISO データ
体積抵抗率 1E11 / 1E11 Ohm*m IEC 62631-3-1
表面抵抗率 * / 1E12 Ohm IEC 62631-3-2
耐電圧 34 / 34 kV/mm IEC 60243-1
耐トラッキング性 - / 600 - IEC 60112
その他の特性.乾燥/調湿単位テスト基準
吸水率 3 / * % Sim. to ISO 62
吸湿率 1.5 / * % Sim. to ISO 62
密度 1000 / - kg/m³ ISO 1183
機能
 粘度せん断速度. , Grilamid TR 90 UV LS natural, PAMACM12, EMS-GRIVORY
 せん断応力-せん断速度. , Grilamid TR 90 UV LS natural, PAMACM12, EMS-GRIVORY
 せん断弾性率-温度. , Grilamid TR 90 UV LS natural (調湿), PAMACM12, EMS-GRIVORY
 応力-ひずみ. , Grilamid TR 90 UV LS natural (調湿), PAMACM12, EMS-GRIVORY
 割線弾性率−ひずみ. , Grilamid TR 90 UV LS natural (調湿), PAMACM12, EMS-GRIVORY
 pvT , Grilamid TR 90 UV LS natural, PAMACM12, EMS-GRIVORY
特殊な特性
成形加工法.
射出成形., その他の押出成形.
納入形状.
顆粒., ナチュラルカラー
添加剤.
離型剤.
特殊な特性.
光安定化., 紫外線安定化., 透明.
Certifications
Food contact, Food approval FDA 21 CFR
アプリケーション
自動車, 電気電子, スポーツ用品
領域別の利用可能性
その他の情報
村遜速揃
PREPROCESSING
Max. water content : <= 0.08 %
PROCESSING
Melt temperature : 270 °C
Mould wall temperature : 60-80 °C
Holding pressure : 300-600 bar
Screw : 50-100 rpm
Back pressure : 1-15 bar
Injection speed : 3
(1=slow, 3=medium, 5=fast)

Please consider the information about the application of the materials.
その他の押出成形.
-- PIPE EXTRUSION --
-- SHEATING --
PROCESSING
Melt temperature : 250-270 °C
Feeding bush : 60-90
Barrel temp. profile : 240-250 °C
Head temp. : 250-240 °C

Please consider the information about the application of the materials.
耐薬品性
5wt%酢酸 (23゚C)
10wt%クエン酸 (23゚C)
10wt%乳酸 (23゚C)
36wt%塩酸 (23゚C)
40wt%硝酸 (23゚C)
38wt%硫酸 (23゚C)
5wt%硫酸 (23゚C)
40wt%硝酸 (23゚C)
塩基
35wt%水酸化ナトリウム (23゚C)
1wt%水酸化ナトリウム (23゚C)
10wt%水酸化アンモニウム (23゚C)
アルコール
イソプロピルアルコール23℃ (23゚C)
メタノール 23℃ (23゚C)
エタノール 23℃ (23゚C)
炭化水素
ヘキサン (23゚C)
トルエン (23゚C)
イソオクタン (23゚C)
ケトン系溶剤
アセトン (23゚C)
エーテル溶剤
ジエチルエーテル (23゚C)
鉱油
SAE 10W40 マルチグレードモーターオイル (23゚C)
SAE 10W40 マルチグレードモーターオイル (130゚C)
SAE 80/90 ハイポイドギアオイル (130゚C)
絶縁油 (23゚C)
標準燃料
ISO 1817液1 (60゚C)
ISO 1817液2 (60゚C)
ISO 1817液3 60℃ (60゚C)
ISO 1817液4 (60゚C)
標準燃料(ISO 1817液C)アルコールなし (23゚C)
標準燃料(ISO 1817液4)アルコールあり (23゚C)
ディーゼル燃料(ISO 1817液F) (23゚C)
ディーゼル燃料(ISO 1817液F) (90゚C)
ディーゼル燃料(ISO 1817液F) (>90゚C)
食塩水
10wt%塩化ナトリウム (23゚C)
10wt%次亜塩素酸ナトリウム (23゚C)
20wt%炭酸ナトリウム (23゚C)
2wt%炭酸ナトリウム (23゚C)
50wt%ジンクロメート (23゚C)
その他
エチルアセテート (23゚C)
過酸化水素 (23゚C)
DOT No.4ブレーキ液 (130゚C)
50wt%エチレングリコール水溶液 (108゚C)
1wt%ノニルフェノキシ-ポリエチレノキシ-エタノール水... (23゚C)
オレイン酸50%+オリーブオイル50% (23゚C)
水 (23゚C)
純水 (90゚C)
5wt%フェノール溶液 (23゚C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.