Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ULTEM™ Resin 1000F - PEI - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for ULTEM™ Resin 1000F:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultem datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
ULTEM 1000F Resin is an unreinforced amorphous polyetherimide (PEI) resin that may offer a high glass transition temperature (Tg) of 217°C and global food compliance (FDA, CN, EC). Features are excellent mechanical, electrical and dimensional properties up to high temperatures. The material provides low staining, microwave transparent and cold to the touch solutions. The material may offer very good chemical resistance for an amorphous material and is inherently flame retardant offering UL94 V0 and 5V ratings. The material is RoHS compliant. The base material is transparent amber colored but is also available in custom colors - transparent and opaque.

UL Yellow Card Link E121562-101048254
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 13 cm³/10min ISO 1133
温度 360 °C -
荷重 5 kg -
ASTM数据
メルトフローレイト, MFI 9 g/10min ASTM D 1238
温度 337 °C -
荷重 6.6 kg -
機械的特性単位テスト基準
ISO データ
引張弾性率 3200 MPa ISO 527
降伏応力 110 MPa ISO 527
降伏ひずみ 6 % ISO 527
破壊ひずみ 50 % ISO 527
曲げ弾性率 3300 MPa ISO 178
ノッチ付きシャルピー衝撃強さ, +23°C 4 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30゚C 4 kJ/m² ISO 179/1eA
Izod impact strength, +23°C, 4mm N kJ/m² ISO 180/1U
Izod impact strength, -30°C, 4mm N kJ/m² ISO 180/1U
ノッチ付きアイゾット衝撃強さ, +23°C, 4mm 6 kJ/m² ISO 180/1A
ノッチ付きアイゾット衝撃強さ, -30°C, 4mm 6 kJ/m² ISO 180/1A
ロックウェル硬度 M 106 - ISO 2039-2
Ball indentation hardness 140 MPa ISO 2039-1
ASTM数据
引張弾性率 3350 MPa ASTM D 638
降伏応力 115 MPa ASTM D 638
降伏点伸び 7 % ASTM D 638
破断伸び 60 % ASTM D 638
曲げ弾性率 3200 MPa ASTM D 790
ロックウェル硬度 M 109 - ASTM D 785
Taber耐摩耗性 10 mg/1000 cycles ASTM D 1044
ノッチ付きIzod衝撃強さ, 1/8 in 53 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 50 J/m ASTM D 256
温度 -30 °C -
アイゾット衝撃試験, 1/8 in 1800 J/m ASTM D 256
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 192 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 209 °C ISO 75-1/-2
ビカット軟化温度, A 215 °C ISO 306
ビカット軟化温度, B 211 °C ISO 306
ビカット軟化温度, 120°C/h 50N 212 °C ISO 306
厚さhでの燃焼性 V-2 class IEC 60695-11-10
試験片の厚さ 0.4 mm -
厚さhでの燃焼性 5V 5VA class IEC 60695-11-20
試験片の厚さ 3.0 mm -
熱伝導率 0.22 W/(m K) DIN 52616
ASTM数据
DTUL @ 66 psi 207 °C ASTM D 648
DTUL @ 264 psi 190 °C ASTM D 648
ビカット軟化温度 211 °C ASTM D 1525
熱伝導率, ソリッド 0.0317 W/(m K) ASTM C 177
電気的特性.単位テスト基準
ISO データ
比誘電率, 1MHz 2.9 - IEC 62631-2-1
誘電正接, 1MHz 60 E-4 IEC 62631-2-1
表面抵抗率 >1E15 Ohm IEC 62631-3-2
耐電圧 33 kV/mm IEC 60243-1
耐トラッキング性 150 - IEC 60112
ASTM数据
耐電圧, 短い時間 19.7 kV/mm ASTM D 149
体積抵抗率 >1E15 Ohm*cm ASTM D 257
その他の特性.単位テスト基準
吸水率. 1.25 % Sim. to ISO 62
密度. 1270 kg/m³ ISO 1183
密度 1270 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 150 °C -
Pre-drying - Time 4 - 6 h -
Processing humidity ≤0.02 % -
樹脂温度 350 - 410 °C -
金型温度 135 - 180 °C -
Zone 1 330 - 400 °C -
Zone 2 340 - 405 °C -
Zone 3 345 - 415 °C -
Back pressure 0.3 - 0.7 MPa -
Processing Recommendation Extrusion単位テスト基準
Pre-drying - Temperature 140 - 150 °C -
Pre-drying - Time 4 - 6 h -
Processing humidity ≤0.02 % -
樹脂温度 320 - 355 °C -
金型温度 65 - 175 °C -
Zone 1 350 - 325 °C -
Zone 2 330 - 355 °C -
Zone 3 330 - 355 °C -
Zone 4 330 - 355 °C -
Zone 5 330 - 355 °C -
特殊な特性
成形加工法.
射出成形., フィルム押出成形., 異形押出成形., ブロー成形., Additive Manufacturing
特殊な特性.
透明.
耐薬品性
General Chemical Resistance
Certifications
Food contact, Food approval FDA 21 CFR, RoHS
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.