Processing/Physical Characteristics | 値 | 単位 | テスト基準 |
Other Standards[S] |
メルトフローレイト, MFI |
12 |
g/10min |
ASTM D 3307 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
機械的特性 | 値 | 単位 | テスト基準 |
ASTM数据 |
曲げ弾性率 |
590 |
MPa |
ASTM D 790 |
ショア硬さD |
55 |
- |
ASTM D 2240 |
Other Standards[S] |
引張強度 |
25 |
MPa |
ASTM D 3307 |
破断伸び |
300 |
% |
ASTM D 3307 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
熱的特性 | 値 | 単位 | テスト基準 |
ASTM数据 |
UL94 燃焼性 |
V-0 |
- |
UL 94 |
酸素指数 |
95 |
% |
ASTM D 2863 |
Other Standards[S] |
溶融温度 |
305 |
°C |
ASTM D 4591 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
電気的特性. | 値 | 単位 | テスト基準 |
ASTM数据 |
耐電圧, 短い時間 |
80 |
kV/mm |
ASTM D 149 |
誘電正接, 1 MHz |
0.0002 |
- |
ASTM D 150 |
比誘電率, 1 MHz |
2.03 |
- |
ASTM D 150 |
体積抵抗率 |
1E18 |
Ohm*cm |
ASTM D 257 |
その他の特性. | 値 | 単位 | テスト基準 |
吸水率, 24hr |
0.03 |
% |
ASTM D 570 |
密度 |
2150 |
kg/m³ |
ASTM D 792 |
特殊な特性
成形加工法.
射出成形., フィルム押出成形., Pipe/Tube Extrusion, 異形押出成形., その他の押出成形., トランスファー成形., Compression Molding
納入形状.
ペレット.
特殊な特性.
紫外線安定化., 熱安定化.
な特性
Good Drawdown, Low Smoke, Melt Strength, Thermal Stability, Tribologic Grade
耐薬品性
General Chemical Resistance
アプリケーション
電気電子, 汎用
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com