Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® PC Resin PC1000 - Asia - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® PC Resin PC1000 - Asia:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
PC1000 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. It is available exclusively at www.sabicpc.com.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 9 cm³/10min ISO 1133
温度 300 °C -
荷重 1.2 kg -
ASTM数据
メルトフローレイト, MFI 10 g/10min ASTM D 1238
温度 300 °C -
荷重 1.2 kg -
機械的特性単位テスト基準
ISO データ
引張弾性率 2350 MPa ISO 527
降伏応力 63 MPa ISO 527
降伏ひずみ 6 % ISO 527
破壊ひずみ 50 % ISO 527
曲げ弾性率 2300 MPa ISO 178
ロックウェル硬度 R 120 - ISO 2039-2
ASTM数据
引張弾性率 2350 MPa ASTM D 638
降伏応力 63 MPa ASTM D 638
降伏点伸び 6 % ASTM D 638
破断伸び 70 % ASTM D 638
曲げ弾性率 2300 MPa ASTM D 790
ロックウェル硬度 R 120 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 800 J/m ASTM D 256
アイゾット衝撃試験, 1/8 in N J/m ASTM D 256
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 127 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 138 °C ISO 75-1/-2
ビカット軟化温度, B 143 °C ISO 306
1.5mm厚さでの燃焼性 V-2 class IEC 60695-11-10
試験片の厚さ 1.5 mm -
熱伝導率 0.2 W/(m K) DIN 52616
ASTM数据
DTUL @ 66 psi 138 °C ASTM D 648
DTUL @ 264 psi 127 °C ASTM D 648
ビカット軟化温度 143 °C ASTM D 1525
熱伝導率, ソリッド 0.0288 W/(m K) ASTM C 177
電気的特性.単位テスト基準
ISO データ
比誘電率, 1MHz 3 - IEC 62631-2-1
誘電正接, 100Hz 10 E-4 IEC 62631-2-1
誘電正接, 1MHz 100 E-4 IEC 62631-2-1
体積抵抗率 >1E13 Ohm*m IEC 62631-3-1
耐電圧 27 kV/mm IEC 60243-1
ASTM数据
耐電圧, 短い時間 27 kV/mm ASTM D 149
誘電正接, 60 Hz 0.001 - ASTM D 150
誘電正接, 1 MHz 0.01 - ASTM D 150
比誘電率, 60 Hz 3 - ASTM D 150
比誘電率, 1 MHz 3 - ASTM D 150
体積抵抗率 1E15 Ohm*cm ASTM D 257
光学特性単位テスト基準
ASTM数据
ヘイズ 0.8 % ASTM D 1003
視感透過率 90 % ASTM D 1003
くっせつりつ 1.59 - ASTM D 542
その他の特性.単位テスト基準
吸水率. 0.35 % Sim. to ISO 62
密度. 1200 kg/m³ ISO 1183
吸水率, 平衡 0.35 % ASTM D 570
密度 1200 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature ≤120 °C -
Pre-drying - Time 2 - 4 h -
樹脂温度 280 - 310 °C -
金型温度 80 - 110 °C -
Zone 1 260 - 280 °C -
Zone 2 270 - 290 °C -
Zone 3 280 - 310 °C -
Nozzle temperature 270 - 290 °C -
特殊な特性
特殊な特性.
紫外線安定化., 熱安定化.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.