Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® LLDPE R50035EE - (PE-LLD) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® LLDPE R50035EE:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
SABIC® LLDPE R50035EE is a LLDPE copolymer that provides good stress crack resistance, rigidity, toughness, gloss and very low warpage. The resin contains UV stabilizer. It is recommended that SABIC® LLDPE R50035EE is grinded before use in rotational moulding applications. Typical Applications. SABIC® LLDPE R50035EE is used for rotational moulding of large industrial and agricultural tanks, trash containers and chemical shipping drums. Because of its good mechanical properties and low warpage, it is used for injection moulding of screw closures, caps and housewares. SABIC® LLDPE R50035EE is UV stabilised; which provides good protection for the final product. Processing conditions. Oven temperature °C (°F) = 315 (600) Typical processing temperature for injection moulding machines: 210 - 240 °C. Mechanical properties. Test specimens are prepared from compression moulded sheet made according to ASTM D-1928, procedure C. This product is not intended for and must not be used in any pharmaceutical/medical applications.
Processing/Physical Characteristics単位テスト基準
ASTM数据
メルトフローレイト, MFI 5 g/10min ASTM D 1238
温度 190 °C -
荷重 2.16 kg -
機械的特性単位テスト基準
ISO データ
ショア硬さD 66 - ISO 7619-1
ASTM数据
降伏応力 16 MPa ASTM D 638
破壊応力 17 MPa ASTM D 638
破断伸び 590 % ASTM D 638
曲げ強さ 13 MPa ASTM D 790
熱的特性単位テスト基準
ASTM数据
ビカット軟化温度 114 °C ASTM D 1525
その他の特性.単位テスト基準
密度 933 kg/m³ ASTM D 792
特殊な特性
成形加工法.
射出成形., 回転成形
特殊な特性.
紫外線安定化.
な特性
High Gloss, Low Warpage, Copolymer
耐薬品性
Environmental Stress Crack Resistance
アプリケーション
パッケージング
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.