Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of LUTENE XL2700BK TR - PE - LG Chem
unit conversion, PDF datasheet print, comparison with other plastics
Check here, which other Lutene datasheets, application examples or technical articles are available in Material Data Center
LUTENE® XL2700BK TR was specially designed crosslinkable semi-conductive compound for easy strippable insulation shielding of medium and high voltage power cable.
LUTENE® XL2700BK TR provides an excellent stripping property, lower and consistent stripping force over a wide temperature range without tearing, leaving a clean insulation surface. Especially LUTENE® XL2700BK TR has an excellent tree retardant propety.
機械的特性 | 値 | 単位 | テスト基準 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ASTM数据 | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
引張強度 | 14.7 | MPa | ASTM D 638 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
破断伸び | 300 | % | ASTM D 638 |
電気的特性. | 値 | 単位 | テスト基準 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Other Standards[S] | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
体積抵抗率 | 100 | Ohm*cm | ASTM D 991 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
その他の特性. | 値 | 単位 | テスト基準 |
密度 | 1160 | kg/m³ | ASTM D 792 |
Moisture Content | 0.05 | % | - |
Processing Recommendation Extrusion | 値 | 単位 | テスト基準 |
Pre-drying - Temperature | 40 | °C | - |
樹脂温度 | 80 - 120 | °C | - |
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.