Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEXAN™ Copolymer EXL9132 - Asia - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for LEXAN™ Copolymer EXL9132 - Asia:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lexan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA.

UL Yellow Card Link E207780-465637
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 16 cm³/10min ISO 1133
温度 300 °C -
荷重 1.2 kg -
ASTM数据
メルトフローレイト, MFI 17 g/10min ASTM D 1238
温度 300 °C -
荷重 1.2 kg -
機械的特性単位テスト基準
ISO データ
引張弾性率 2200 MPa ISO 527
降伏応力 59 MPa ISO 527
降伏ひずみ 5 % ISO 527
破壊応力 55 MPa ISO 527
破壊ひずみ 50 % ISO 527
曲げ弾性率 2300 MPa ISO 178
シャルピー衝撃強さ, +23°C, 3mm N kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C, 3mm N kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C, 3mm 60 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C, 3mm 25 kJ/m² ISO 179/1eA
アイゾット衝撃試験, +23°C N kJ/m² ISO 180/1U
ノッチ付きアイゾット衝撃強さ, +23°C, 3mm 55 kJ/m² ISO 180/1A
ノッチ付きアイゾット衝撃強, -30°C, 3mm 20 kJ/m² ISO 180/1A
Ball indentation hardness 95 MPa ISO 2039-1
ASTM数据
引張弾性率 2260 MPa ASTM D 638
降伏応力 58 MPa ASTM D 638
破壊応力 58 MPa ASTM D 638
降伏点伸び 5.8 % ASTM D 638
破断伸び 103 % ASTM D 638
曲げ弾性率 2330 MPa ASTM D 790
ノッチ付きIzod衝撃強さ, 1/8 in 731 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 560 J/m ASTM D 256
温度 -30 °C -
熱的特性単位テスト基準
ISO データ
ビカット軟化温度, B 143 °C ISO 306
ビカット軟化温度, 120°C/h 50N 144 °C ISO 306
1.5mm厚さでの燃焼性 V-0 class IEC 60695-11-10
試験片の厚さ 1.5 mm -
厚さhでの燃焼性 5V 5VA class IEC 60695-11-20
試験片の厚さ 3.0 mm -
グローワイヤ燃焼性指数 (GWFI) 960 °C IEC 60695-2-12
グローワイヤ着火温度 (GWIT) 825 °C IEC 60695-2-13
GWIT - 試験片の厚さ 3 mm -
ASTM数据
DTUL @ 66 psi 136 °C ASTM D 648
DTUL @ 264 psi 123 °C ASTM D 648
ビカット軟化温度 143 °C ASTM D 1525
電気的特性.単位テスト基準
ISO データ
比誘電率, 1MHz 2.7 - IEC 62631-2-1
誘電正接, 1MHz 100 E-4 IEC 62631-2-1
耐トラッキング性 175 - IEC 60112
その他の特性.単位テスト基準
吸水率. 0.35 % Sim. to ISO 62
吸湿率 0.15 % Sim. to ISO 62
密度. 1190 kg/m³ ISO 1183
密度 1180 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 120 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.02 % -
樹脂温度 295 - 315 °C -
金型温度 70 - 95 °C -
Zone 1 270 - 295 °C -
Zone 2 280 - 305 °C -
Zone 3 295 - 315 °C -
Screw speed 40 - 70 rpm -
Back pressure 0.3 - 0.7 MPa -
特殊な特性
成形加工法.
射出成形.
添加剤.
難燃剤.
特殊な特性.
難燃.
領域別の利用可能性
アジア/太平洋地域.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.