Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Grilon CR 8 natural - PA612 - EMS-GRIVORY | a unit of EMS-CHEMIE AG

Material Data Center offers the following functions for Grilon CR 8 natural:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Grilon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Product-nomenclature: ISO 16396-PA6/12,,FT,C16-020

 

Co Polyamide

Product Attributes

  Highly flexible, High viscosity, Highly transparent, Barrier material

Markets

  Packaging
  Oriented film

Approvals

  Food Contact
  EU Requirements
Processing/Physical Characteristics乾燥/調湿単位テスト基準
ISO データ
メルトボリュームレイト, MVR 120 / * cm³/10min ISO 1133
温度 275 / * °C -
荷重 5 / * kg -
機械的特性乾燥/調湿単位テスト基準
ISO データ
引張弾性率 - / 500 MPa ISO 527
熱的特性乾燥/調湿単位テスト基準
ISO データ
溶融温度, 10°C/min 190 / * °C ISO 11357-1/-3
光学特性乾燥/調湿単位テスト基準
ISO Data
光沢度, 60° 130 / * - ISO 2813
その他の特性.乾燥/調湿単位テスト基準
吸水率 8 / * % Sim. to ISO 62
吸湿率 2 / * % Sim. to ISO 62
密度 1100 / - kg/m³ ISO 1183
機械的特性(ィルム)乾燥/調湿単位テスト基準
ISO データ
降伏応力, 平行 28 / * MPa ISO 527-3
降伏応力, 直角 28 / * MPa ISO 527-3
降伏ひずみ, 平行 10 / * % ISO 527-3
降伏ひずみ, 直角 10 / * % ISO 527-3
最大ひずみ, 平行 900 / * % ISO 527-3
最大ひずみ, 直角 900 / * % ISO 527-3
エルメンドルフ引裂抵抗, 平行 20 / * N ISO 6383-2
エルメンドルフ引裂抵抗, 直角 20 / * N ISO 6383-2
トラウザー引裂抵抗, 平行 65 / * N/mm ISO 6383-1
トラウザー引裂抵抗, 直角 65 / * N/mm ISO 6383-1
水蒸気透過度, 23°C/85%r.h. 15 / * g/(m²*d) ISO 15106-1/-2
酸素透過度., 23゚C/0%r.h. 80 / * cm³/(m²*d*bar) ISO 15105-1/-2
酸素透過度., 23°C/85%r.h. 90 / * cm³/(m²*d*bar) ISO 15105-1/-2
二酸化炭素透過度, 23°C/0%r.h. 300 / * cm³/(m²*d*bar) ISO 15105-1/-2
二酸化炭素透過度, 23°C/85%r.h. 800 / * cm³/(m²*d*bar) ISO 15105-1/-2
特殊な特性
成形加工法.
フィルム押出成形., その他の押出成形., 熱成形.
納入形状.
顆粒., ナチュラルカラー
特殊な特性.
透明.
な特性
Barrier Properties, Copolymer
Certifications
Food contact
アプリケーション
パッケージング
領域別の利用可能性
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.