Caratteristiche Fisiche | Valore | Unitá | Norma del test |
Other Standards[S] |
Indice di fluidità a caldo, MFI |
6 |
g/10min |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
Proprietà Meccaniche | Valore | Unitá | Norma del test |
Other Standards[S] |
Modulo a flessione |
2392 |
MPa |
|
Resistenza alla flessione |
55.2 |
MPa |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
Proprietà Termiche | Valore | Unitá | Norma del test |
ASTM Data |
Temperatura di fusione |
210 |
°C |
ASTM D 3418 |
Proprietà Ottiche | Valore | Unitá | Norma del test |
ASTM Data |
Brillantezza |
90[1] |
- |
ASTM D 2457 |
Opacità |
2.1 |
% |
ASTM D 1003 |
Altre Proprietà | Valore | Unitá | Norma del test |
Densità |
1240 |
kg/m³ |
ASTM D 792 |
Proprietà Meccaniche (Film) | Valore | Unitá | Norma del test |
ASTM Data |
Modulo a trazione, lung. |
3310 |
MPa |
ASTM D 882 |
Resistenza alla trazione, lung. |
110 |
MPa |
ASTM D 882 |
Allungamento a rottura, lung. |
160 |
% |
ASTM D 882 |
Caratteristiche
Processabilità e Forma di Forni
Additive Manufacturing
Forma fisica disponibile
Monofilament
Caratteristiche speciali
Alto urto o modificato all'urto
Caratteristiche
Buona adesione
Certifications
Contiene risorse rinnovabili
Disponibilità geografica
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.