Caracteristicas de procesamiento y fisicas | Valor | Unidades | Método de ensayo |
Other Standards[S] |
Índice de fluidez, MFI |
6 |
g/10min |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propiedades mecánicas | Valor | Unidades | Método de ensayo |
Other Standards[S] |
Módulo de flexión |
2392 |
MPa |
|
Resistencia a la flexión |
55.2 |
MPa |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propiedades térmicas | Valor | Unidades | Método de ensayo |
ASTM Data |
Temperatura de fusión |
210 |
°C |
ASTM D 3418 |
Propiedades opticas | Valor | Unidades | Método de ensayo |
ASTM Data |
Brillo |
90[1] |
- |
ASTM D 2457 |
Opacidad |
2.1 |
% |
ASTM D 1003 |
Otras propiedades | Valor | Unidades | Método de ensayo |
Densidad |
1240 |
kg/m³ |
ASTM D 792 |
Propiedades mecánicas (Film) | Valor | Unidades | Método de ensayo |
ASTM Data |
Módulo de tracción, long. |
3310 |
MPa |
ASTM D 882 |
Esfuerzo de tracción, long. |
110 |
MPa |
ASTM D 882 |
Alargamiento a la rotura, long. |
160 |
% |
ASTM D 882 |
Características
Procesamiento y forma de entrega
Additive Manufacturing
Forma de suministro
Monofilamento
Características especiales
Alto impacto o modificado al impacto
Características
Buenas propiedades de adhesión
Certifications
Contiene recursos renovables
Disponibilidad regional
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.