Vestolen - PE-HD, PP - Saudi Basic Industries Corp. (Sabic)
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Vestolen" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...ntially, which is especially advantageous when processing temperature-sensitive materials. Material Degradation within Limits The mild treatment of the material in the ring extruder was demonstrated when processing a standard polypropylene (grade: Vestolen 17M10, manufacturer: DSM Polyolefine GmbH, Gelsenkirchen). The operating parameters of a co-rotating twin-screw extruder belonging to the polypropylene manufacturer was used for comparative data. The process section of the ring extruder had ...
Kunststoffe international, 2005-11-21, Compounding: Maximising Use of Machine Potential
...tice The graphs in Fig.7 plot the calculated against the measured energy. Generally speaking, good correlation was achieved for all materials. Deviations occurred primarily at low outputs coupled with high speeds. These were most noticeable with Vestolen P7000 and PE-LLD. At the above-mentioned operating points, there was high dissipation, so that the interfacial temperature between the melt and barrel wall differed significantly from the actual barrel wall temperature. This interfacial temperat...
Kunststoffe international, 2005-11-21, Improved Injection Moulding Simulation
...ariable range, and was therefore held constant. Thin sections were taken from these panels along the flow path and the outer layer thicknesses measured by polarisation microscopy. A typical layer structure of an injection-moulded panel of PP (grade: Vestolen P 7000, manufactured by: DSM Petrochemicals) is shown in Fig. 5; also see [10, 11]. The measured outer layer thicknesses are shown in Fig. 6. The results show that, - a) at constant injection time and increasing melt temperature, and - b) at...
Kunststoffe international, 2005-11-21, Injection Moulding Simulation: Balancing a Family Mould
...nt in the simulation. The Non-balanced State With the above runner dimensions and the computation parameters set out below: - program: Cadmould cmv 6.3, - calculation: multilaminar, compressible, non-isothermal, - moulding compound: PP Vestolen 5200, - melt temperature: 240°C, - mould temperature: 50°C, - volume flow: 40cm³/s, - holding pressure (HP): 150bar, - switchover to HP at: 100% full the melt reaches all three sheets simultaneously, but complete filling of the three cavities is achieved...
Kunststoffe international, 2005-11-21, Polypropylene
...ket. Targor was formed mid 1997, combining the PP activities of BASF and Hoechst AG. It became the second largest European producer with more than 1.5 million tonnes capacity, just behind then European leader Montell (Himont-Shell JV). DSM took over Vestolen GmbH early 1998 and Dow started mid 1998 its first European PP production unit, located in Schkopau. A few months later, Borealis and PCD joint forces. A new wave of restructuring started early in the new millennium. Basell was formed in Oct...
Kunststoffe international, 2007-12-17, Logistics and Know-how Rule the Market
...ver, it is due to bring ecological as well as economic benefit. Ticona has recently reduced its price for PP Celstran, which is used as a carrier material in many vehicles today. PE: Pipes and Grass At the K show, Sabic introduced the Vestolen A 6060 R polyethylene, which is designed for water ducts and is being applied in Montenegro. Borsafe is the name of a Borealis product designed to manufacture pipes of high qualities and stiffnesses, serving the same purpose. Both of these systems are PE...
Kunststoffe international, 2011-10-17, Polypropylene (PP)
...reduces deposits inside the pipe. For over 30 years, hot and cold water installations have used pipes made from random polypropylene copolymers (PP-R) due to their good resistance to heat and pressure; examples of standard materials here are Vestolen P9421 (Sabic) and Borealis RA130. The new PP-RCT class of materials enables pipes to be used at higher pressures or their wall thickness to be reduced. The polymer beta PP-R RA7050 (Borealis) is tailormade in terms of molecular weight distribution a...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.