Tenax - PAN - Teijin Chemicals Ltd
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Tenax" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...ated defect-free by this method with only one linear gate. To characterise the influence of the seam, unidirectional carbon-fibre fabrics made by epo GmbH, Willich/Germany (Udo UD CST 170/600, Udo UD CS 240/348, fibre grade: Tenax STS 5631 24K 1600tex) were sewn and impregnated by the resin infusion process. The test sheets so produced have a very high average volume content of 64% and are currently undergoing tensile tests at ilb. Micrographs (Fig.8) show the excellent, defect-free, impregnated...
Kunststoffe international, 2005-11-21, Definition of Terms: From the Plant to the Natural Fibre-reinforced Part
...by the problem of confusion of different types of fibres. Ambiguous, imprecise terminology makes it difficult to clarify the legal problems in the event of disputes. For example, the common term “New Zealand flax” (fibres of the plant Phormium tenax J.R.) does not refer to flax from New Zealand, but is botanically speaking a completely different type of fibre. It is difficult to complain about a trader selling these fibres to his customers as flax, since even the import statistics categorise the...
Kunststoffe international, 2005-11-21, Fibre Composite Parts: Automated Preform-RTM Production
...s launched in March 2001 and is running until the end of August 2004. A detailed presentation may be found under www.ivw.uni-kl.de/propreformrtm/ The Authors Dr.-Ing. Markus Schneider, born in 1969, is Head of Process Development at Tenax Fibers; markus.schneider@tenax-fibers.com Dr.-Ing. Christian Weimer, born in 1972, is Group Leader of the Processing Technology Department at the Institut für Verbundwerkstoffe GmbH (Composites Institute); weimer@ivw.uni-kl.de Dipl.-Ing. (FH) Franz Hägle, born...
Kunststoffe international, 2005-11-21, Fibre Composites in the Global Limelight
...applications is to be extended by means of forward integration, i. e. through the acquisition of component producers (e. g. SP-Systems, Newport/Great Britain). In order to cater for the trend towards processing less expensive carbon fibre tows, the Tenax company of Wuppertal/Germany also has a low-cost 24K roving in its supply range. In the field of natural fibre reinforcement, an increased number of specific series applications are to be found with thermoplastic matrices (e. g. LST, Lynnwoodrid...
Kunststoffe international, 2006-02-22, Carbon-fibre-reinforced Plastics (CRP): The Black Gold of Lightweight Building
...Kunststoffe plast europe 92 (2002) 11, pp. 43-47 5 Mitschang, P.: Schlüsseltechnologien für die Preform-LCM-Prozesskette. 8. Internationale AVK-Tagung , B9/1-9/12, Baden-Baden 2005 6 www.hexcel.com 7 www.spsystems.com 8 www.tohotenax-eu.com 9 www.huntsman.com 10 www.hexionchem.com 11 www.dsm.com 12 www.reichhold.com 13 Marsh, G.: Composites lift off in primary aerostructures. Reinforced Plastics 48 (2004) 4, pp. 22-27 14 www.eads.com 15 Projekte zu CFK-Flugzeugstrukturen (Auswahl): TANGO, ALCAS...
Kunststoffe international, 2012-06-25, CRP Components with Class A Surfaces
...e: 405 g/m2; STS industrial fibers), on quadraxial bonded fabrics (0°/90°/+ 45°/ - 45°; grammage: 1620 g/m2; STS industrial fibers) and on woven fabrics (grammage: 200 g/m2; HTA industrial fiber) from carbon fibers (manufacturer: Toho Tenax Europe GmbH, Wuppertal, Germany). Mold temperature, as well as a temperature gradient, the type of preform, the amount and type of dwell pressure, the content of fiber volume, as well as surface mats, were considered as to their effects on surface qualities. ...
Kunststoffe international, 2012-11-26, Fibers and Nano-Fillers Combined
...l Ministry of Economics and Technology, following a decision of the German Bundestag. Our thanks to all institutions. We would like to thank BASF SE, Coperion GmbH, Dow Europe GmbH, Rockwood Clay Additives GmbH, PPG Industries Fiber Glass B.V., Toho Tenax Europe GmbH and Nanocyl S.A. for providing experimental material and equipment. Fig. 1. Screw configuration and processing parameters for the production of short fiber reinforced nanocomposites from polypropylene, glass fibers and layered silic...
Kunststoffe international, 2012-11-26, Lighter in the Air, in the Wind and on the Road
... also Table 1) [21]. In addition to neat resins, the interlaminar fracture toughness Mode I (GIc) in unidirectionally reinforced carbon fiber composites has been extensively studied. For this, prepregs (carbon fibers: Toho Tenax-E HTA 5131, 800 Tex F6000 TO (Toho Tenax Co., Ltd., Tokyo, Japan)) were produced from the resins containing electron beam initiators. The results in Figure 8 show that the electron-beamcured composite, despite toughening, has much lower interlaminar fracture toughness ch...
Kunststoffe international, 2017-07-19, A Thicket of Fibers
...cured at 50 °C for three hours. When the composite has been demolded, test specimens can be milled out for mechanical tests. Strength and Elastic Modulus of the CompositesInitial test results (with carbon fibers: HTC 124, manufacturer: Toho Tenax Europe GmbH, Wuppertal, Germany) show slight anisotropy in the machine direction of the wet-laying unit. Specimens measured transverse to the machine direction attain 90 % of the tensile strength and 95 % of the elastic modulus achieved by the specimen...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.