Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of SABIC® PP FPC100 - PP - Saudi Basic Industries Corporation (SABIC)
Material Data Center offers the following functions for SABIC® PP FPC100:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
Testo del prodotto
SABIC® PP FPC100 has been developed as a new member of the SABIC® PP FLOWPACT range dedicated to the thin wall packaging market. It is nucleated and is characterized by a high crystallization temperature and excellent flow behaviour in combination with a nice stiffness to impact balance.
This grade is typically used for high-speed injection moulding and it enables very cost efficient processing on the basis of easy mould filling and very short cycle times. It has a very good antistatic performance and permitseasy demoulding.This material is typically used in thin wall packing applications both for food and non-food segments. This includes yellow fats/margarine tubs, dairy packaging and housewares. The grade has an excellent dimensional stability what is crucial for the thin wall packaging market.
Health, Safety and Food Contact regulations:Material Safety Data Sheets (MSDS) and Product Safety declarations are available on our Internet site
http://www.SABIC.comThe product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/ medical applications.
IMDS 80775790
Proprietà Meccaniche | Valore | Unitá | Norma del test |
ISO Data |
Modulo a trazione |
1450 |
MPa |
ISO 527 |
Carico unitario a trazione |
25 |
MPa |
ISO 527 |
Deformazione a snervamento |
4 |
% |
ISO 527 |
Resist. urto Charpy con intaglio, +23°C |
8 |
kJ/m² |
ISO 179/1eA |
Durezza Shore D |
62 |
- |
ISO 7619-1 |
Proprietà Termiche | Valore | Unitá | Norma del test |
ISO Data |
Temp.di inflessione sotto carico, 1.80 MPa |
55 |
°C |
ISO 75-1/-2 |
Temp.di inflessione sotto carico, 0.45 MPa |
95 |
°C |
ISO 75-1/-2 |
Temp.di rammollimento Vicat, A |
150 |
°C |
ISO 306 |
Temp.di rammollimento Vicat, B |
76 |
°C |
ISO 306 |
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Certifications
Contatto con gli alimenti
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.