Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of SABIC® PP 621P - PP - Saudi Basic Industries Corporation (SABIC)
Material Data Center offers the following functions for SABIC® PP 621P:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
Testo del prodotto
SABIC®PP 621P is a newly designed random copolymer polypropylene particularly for cast film applications with high clarity. Products produced out of SABIC® PP 621P have a high clarity, excellent sealing performance and high puncture resistance. The molecular structure of this grade is tailored for high performance processing. SABIC® PP 621P does not contain anti-block and slip agent. A grade with anti-block and slip agent is available as SABIC® PP 622L.
Applications: SABIC PP 621P is typically used in applications like food packaging, lamination film, stationary film, textile packaging, flower packaging, and hygiene packaging. SABIC®PP 621P is also a partner resin of LLDPE for power stretch film to which high holding force is required in order to assure good pallet stability.
Specific applications are: sparkling beverage, building & construction materials and in general unitized heavy goods.
SABIC®PP 621P has a good rheological matching with LLDPE which result in an easy process-ability (see graph on second page).
Health, Safety and Food Contact regulations: SABIC®PP 621P has a Food Contact Declaration. Material Safety Data Sheets (MSDS) and Product Safety
Declarations are available on our Internet site
http://www.sabic.com.
The product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/medical applications. IMDS 80775790
Proprietà Meccaniche | Valore | Unitá | Norma del test |
ISO Data |
Modulo a trazione |
800 |
MPa |
ISO 527 |
Carico unitario a trazione |
25 |
MPa |
ISO 527 |
Deformazione a snervamento |
13 |
% |
ISO 527 |
Proprietà Termiche | Valore | Unitá | Norma del test |
ISO Data |
Temp.di rammollimento Vicat, A |
128 |
°C |
ISO 306 |
Temp.di rammollimento Vicat, B |
63 |
°C |
ISO 306 |
Caratteristiche
Caratteristiche
Copolimero
Certifications
Contatto con gli alimenti
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.