Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL™ Resin EM6100 - Americas - (PPE+PS) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL™ Resin EM6100 - Americas:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
NORYL™ EM6100 is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This grade exhibits a balance of flow/heat/impact, dimensional stability, along with paint adhesion. NORYL EM6100 resin is suitable for the automotive interior market in applications such as HVAC housings and radio components. MS-DB424, WSBM4D844-A9, GMP.PPE.007.

UL Yellow Card Link E121562-221232
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 15 cm³/10min ISO 1133
Temperatura 280 °C -
Carico 5 kg -
ASTM Data
Indice di fluidità a caldo, MFI 15 g/10min ASTM D 1238
Temperatura 280 °C -
Carico 5 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 2050 MPa ISO 527
Carico unitario a trazione 42 MPa ISO 527
Deformazione a snervamento 2.8 % ISO 527
Carico unitario a rottura 40 MPa ISO 527
Deformazione a rottura 50 % ISO 527
Modulo a flessione 2100 MPa ISO 178
Resistenza alla flessione 65 MPa ISO 178
Resist. urto Izod con intaglio, +23°C, 4mm 33 kJ/m² ISO 180/1A
Resist. urto Izod con intaglio, -30°C, 4mm 15 kJ/m² ISO 180/1A
ASTM Data
Modulo a trazione 1900 MPa ASTM D 638
Resistenza alla trazione di snervamento 43 MPa ASTM D 638
Resistenza alla trazione a rottura 40 MPa ASTM D 638
Allungamento a snervamento 3 % ASTM D 638
Allungamento a rottura 65 % ASTM D 638
Modulo a flessione 2100 MPa ASTM D 790
Resistenza all'urto Izod con intaglio, 1/8 in 453 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, basso temperatura 250 J/m ASTM D 256
Temperatura -30 °C -
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 110 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 126 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 119 °C ISO 306
Temp.di rammollimento Vicat, 120°C/h 50N 123 °C ISO 306
Reaz. al fuoco spess.nom. 1.5mm HB class IEC 60695-11-10
Spessore provato 1.5 mm -
ASTM Data
DTUL a 66 psi 124 °C ASTM D 648
DTUL a 264 psi 106 °C ASTM D 648
Altre ProprietàValoreUnitáNorma del test
Densità 1050 kg/m³ ASTM D 792
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 95 - 105 °C -
Pre-essiccamento - Tempo 3 - 4 h -
Umidità del Processo ≤0.02 % -
Temperatura di fusione 265 - 295 °C -
Temperatura dello stampo 65 - 95 °C -
Zona 1 230 - 280 °C -
Zona 2 245 - 290 °C -
Zona 3 255 - 295 °C -
Velocità di Rotazione della Vite 20 - 100 rpm -
Contropressione 0.3 - 0.7 MPa -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Applicazioni
Automotive
Disponibilità geografica
Nord America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.