Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL GTX™ Resin GTX989 - Europe - (PPE+PA*) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL GTX™ Resin GTX989 - Europe:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
NORYL GTX™ 989 resin is a conductive, non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade is optimized for primer-less electrostatic painting. NORYL GTX989 resin exhibits high heat resistance, high impact resistance, and low coefficient of thermal expansion (CTE) of ~9. This material is an excellent candidate for automotive applications such as body panels, tank flaps, fenders, trunk lid, and exterior trim.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 19 cm³/10min ISO 1133
Temperatura 280 °C -
Carico 5 kg -
ASTM Data
Indice di fluidità a caldo, MFI 16 g/10min ASTM D 1238
Temperatura 280 °C -
Carico 5 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 2300 MPa ISO 527
Carico unitario a trazione 60 MPa ISO 527
Deformazione a snervamento 5 % ISO 527
Carico unitario a rottura 55 MPa ISO 527
Deformazione a rottura 40 % ISO 527
Modulo a flessione 2300 MPa ISO 178
Resist. urto Charpy con intaglio, +23°C 22 kJ/m² ISO 179/1eA
Resist. urto Charpy con intaglio, -30°C 15 kJ/m² ISO 179/1eA
Resist. urto Izod con intaglio, +23°C, 4mm 22 kJ/m² ISO 180/1A
Resist. urto Izod con intaglio, -30°C, 4mm 15 kJ/m² ISO 180/1A
ASTM Data
Modulo a trazione 2350 MPa ASTM D 638
Resistenza alla trazione di snervamento 65 MPa ASTM D 638
Resistenza alla trazione a rottura 60 MPa ASTM D 638
Allungamento a snervamento 5 % ASTM D 638
Allungamento a rottura 45 % ASTM D 638
Modulo a flessione 2450 MPa ASTM D 790
Resistenza all'urto Izod con intaglio, 1/8 in 240 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, basso temperatura 180 J/m ASTM D 256
Temperatura -30 °C -
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di rammollimento Vicat, B 195 °C ISO 306
Temp.di rammollimento Vicat, 120°C/h 50N 200 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 90 E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin. , perpend. 90 E-6/K ISO 11359-1/-2
ASTM Data
DTUL a 66 psi 190 °C ASTM D 648
Temp.di rammollimento Vicat 195 °C ASTM D 1525
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'acqua 4.2 % Sim. alla ISO 62
Assorbimento d'umidità 1.2 % Sim. alla ISO 62
Massa volumica 1080 kg/m³ ISO 1183
Densità 1080 kg/m³ ASTM D 792
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 100 - 120 °C -
Pre-essiccamento - Tempo 2 - 3 h -
Umidità del Processo ≤0.07 % -
Temperatura di fusione 290 - 320 °C -
Temperatura dello stampo 100 - 120 °C -
Temperatura - Zona di Alimentazione 60 - 80 °C -
Zona 1 260 - 280 °C -
Zona 2 280 - 300 °C -
Zona 3 290 - 320 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Applicazioni
Automotive
Disponibilità geografica
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.