Material datasheets available free. Online registration at: www.materialdatacenter.com
Chimassorb - Antioxidants, UV-light stabilizers - BASF SE
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Chimassorb" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...racture in the production of a white PE-LLD film with a HALS 3 stabiliser Table 1. Maximum tensile strength resisted by the weld after sealing at different temperatures (light stabilisers from other suppliers mentioned in the text: HALS 1: Chimassorb 944 from Ciba Speciality Chemicals, Basel/Switzerland; HALS 2: Hostavin N 30 from Clariant International, Muttenz/Switzerland; HALS 3: Tinuvin 622 from Ciba Speciality Chemicals, Basel; HALS 4: Uvasil HA 88 from 3V Sigma, Bergamo/Italy) Manufactur...
Kunststoffe international, 2005-11-21, Integrated Solutions
...res is glass-fibre-filled polypropylene. Since the stabiliser systems used to date for these applications can lead to the formation of odours, new solutions were sought. Combinations of Irganox B blends and hindered amides – essentially Chimassorb 119 – were highly temperature resistant. Improved Recycling The European Commission has recently introduced new requirements whereby automotive manufacturers are called upon to considerably increase the share of recyclable material in end-of-life car...
Kunststoffe international, 2010-08-19, Profitable and Faster than the Market
...eptionally high color strength, heat resistance as well as colorfastness in outdoor applications. A long product life even when exposed to strong sunlight is ensured by the lightstabilizing additives from the Chimassorb and Tinuvin families that were initially developed by Ciba and are now part of BASF. According to Reiners, with this integrated approach, not only is the additives product range strengthened; the previous Ciba business within the unit has also gained in importance significantly f...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.