Material datasheets available free. Online registration at: www.materialdatacenter.com
Celazole - PBI - PBI Performance Products, Inc
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Celazole" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...from glass-filled PEEK to withstand temperatures of up to 200°C at 20bar pressure. Product Innovations and Trends In 2006, Victrex introduced its new T-series product range, a proprietary blend based on Victrex PEEK and Celazole PBI. The T-series consists of an unfilled product also available as glass- and carbon-fiber filled pellets as well as a lubricated grade. It is designed to be melt processable and capable of performing in the most demanding high-temperature applications requiring super...
Kunststoffe international, 2008-10-17, Polyaryletherketones (PAEKs)
... can be supplied in widths up to 1,500 mm and a thickness of 6 to 750 µm, with amorphous or semicrystalline morphology, unreinforced or mineral filled. The T-Series, consisting of a number of patent-protected blends based on Victrex PEEK and Celazole polybenzimidazole (PBI), was launched in 2006. This granulate is available unreinforced, reinforced with glass fiber or carbon fiber, and with a slip modification. T-series products can be processed by standard methods for thermoplastics and...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.