Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® PPcompound 8620 - PP - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® PPcompound 8620:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
SABIC® PPcompound 8620 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and good flow with exterior automotive weathering stability. It was originally designed for painted or unpainted automotive bumper fascia applications where a combination of high stiffness and cold temperature ductility is required. IMDS ID: 209747700
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité, MFI 23 g/10min ISO 1133
Température 230 °C -
Charge 2.16 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 1680 MPa ISO 527
Contrainte d'écoulement 17 MPa ISO 527
Déformation au seuil d'écoulement 4.4 % ISO 527
Contrainte à la rupture 11 MPa ISO 527
Déformation à la rupture 39 % ISO 527
Module de flexion, 23°C 1740 MPa ISO 178
Résistance au choc Charpy (entaillé), +23°C 58 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 7 kJ/m² ISO 179/1eA
Résistance au choc Izod avec entaille 6 kJ/m² ISO 180/1A
ASTM Data
Module en traction 1900 MPa ASTM D 638
Module de traction d’élasticité 17 MPa ASTM D 638
Résistance de traction à la rupture 12 MPa ASTM D 638
Allongement d’élasticité 5 % ASTM D 638
Allongement à la rupture 101 % ASTM D 638
Module de flexion 1380 MPa ASTM D 790
Dureté D Shore 54 - ASTM D 2240
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 56 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 100 °C ISO 75-1/-2
Température de ramolliss. Vicat, A 123 °C ISO 306
ASTM Data
DTUL à 66 psi 98 °C ASTM D 648
DTUL à 264 psi 52 °C ASTM D 648
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1030 kg/m³ ISO 1183
Densité 1030 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 80 - 100 °C -
Pré-séchage - temps 2 - 4 h -
Température de la matière fondue 210 - 270 °C -
Température du moule 15 - 60 °C -
Zone 1 190 - 230 °C -
Zone 2 200 - 250 °C -
Zone 3 210 - 270 °C -
Température de la buse 210 - 270 °C -
Contre-pression 1 - 1.5 MPa -
Caractéristiques
Propriétés spéciales
Modifié choc
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com