Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL™ Resin HMC1010 - (PPE+PS)-CF10 - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL™ Resin HMC1010:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
NORYL HMC1010 compound is based on Polyphenylene Ether (PPE) resin containing 10% carbon fiber. Added features of this grade include: Electrically Conductive, Non-Chlorinated, Non-Brominated Flame Retardant.

UL Yellow Card Link E121562-221166
Propriétés mécaniquesValeurUnitéNorme du test
ASTM Data
Module de traction d’élasticité 79 MPa ASTM D 638
Résistance de traction à la rupture 71 MPa ASTM D 638
Allongement à la rupture 3 % ASTM D 638
Dureté Rockwell R 122 - ASTM D 785
Taber abrasion résistance 83 mg/1000 cycles ASTM D 1044
Izod choc avec entaille, 1/8 in 69 J/m ASTM D 256
Résistance au choc Izod, 1/8 in 240 J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Inflammabilité pr. épaisseur h V-1 class IEC 60695-11-10
Epaisseur de l'éprouvette 2.0 mm -
Inflammabilité 5V pr. épaisseur h 5VA class IEC 60695-11-20
Epaisseur de l'éprouvette 2.0 mm -
Propriétés électriquesValeurUnitéNorme du test
ASTM Data
Résistance de la surface 13000 Ohm ASTM D 257
Résistance volumique 8000 Ohm*cm ASTM D 257
Propriétés diversesValeurUnitéNorme du test
Densité 1150 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 90 - 95 °C -
Pré-séchage - temps 3 - 4 h -
L'humidité de traitement ≤0.02 % -
Température de la matière fondue 255 - 280 °C -
Température du moule 65 - 90 °C -
Zone 1 220 - 270 °C -
Zone 2 230 - 275 °C -
Zone 3 245 - 280 °C -
Vitesse de rotation de vis 20 - 100 rpm -
Contre-pression 0.3 - 0.7 MPa -
Caractéristiques
Transformation
Moulage par injection
Additifs
Agent ignifugeant
Propriétés spéciales
Conductivité électrique accrue, Ignifugé
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com