Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of Monprene® CP-17270 - TPE-X - Teknor Apex Co.
unit conversion, PDF datasheet print, comparison with other plastics
Check here, which other Monprene datasheets, application examples or technical articles are available in Material Data Center
The Monprene CP-17200 Filled, High Flow Series of thermoplastic elastomer compounds, with good UV resistance, available in NAT or colors, from 40 to 80 Shore A, are designed specifically for EU consumer product applications requiring a soft, rubber-like feel. Monprene CP-17270 is a medium hardness, medium density grade that is suitable for injection molding and extrusion.
Adheres to PP
Property | Value | Unit | Standard |
---|---|---|---|
Apparent Viscosity (200 °C, 206 1/s) | 107 | Pas | ASTM D3835 |
Caractéristiques des transformations/physiques | Valeur | Unité | Norme du test | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ASTM Data | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Indice de fluidité, MFI | 25 | g/10min | ASTM D 1238 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Température | 230 | °C | - | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Charge | 2.16 | kg | - |
Propriétés mécaniques | Valeur | Unité | Norme du test | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ASTM Data | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Module à 100% allongement | 1.9 | MPa | ASTM D 412 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Module à 300% allongement | 0.87 | MPa | ASTM D 412 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Dureté A Shore | 70 | - | ASTM D 2240 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Compression rémanente, 22 hr @ 73 °F | 31 | % | ASTM D 395 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Compression rémanente, 22 hr @ 158 °F | 55 | % | ASTM D 395 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Résistance de traction à la rupture | 7.6 | MPa | ASTM D 412 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Allongement à la rupture | 800 | % | ASTM D 412 |
Propriétés diverses | Valeur | Unité | Norme du test |
Densité | 1050 | kg/m³ | ASTM D 792 |
Recommandations pour la transformation Moulage par injection | Valeur | Unité | Norme du test |
Pré-séchage - température | 65 | °C | - |
Pré-séchage - temps | 2 - 4 | h | - |
Température de la matière fondue | 199 - 249 | °C | - |
Température du moule | 35 - 49 | °C | - |
Zone 1 | 182 - 232 | °C | - |
Zone 2 | 188 - 238 | °C | - |
Zone 3 | 193 - 243 | °C | - |
Température de la buse | 199 - 249 | °C | - |
Vitesse de rotation de vis | 50 - 100 | rpm | - |
Pressions d'injection | 1.38 - 5.52 | MPa | - |
Contre-pression | 0.172 - 0.689 | MPa | - |
Recommandations pour la transformation Extrusion | Valeur | Unité | Norme du test |
Zone 1 | 182 - 232 | °C | - |
Zone 2 | 188 - 238 | °C | - |
Zone 3 | 193 - 243 | °C | - |
Zone 4 | 199 - 249 | °C | - |
Zone 5 | 199 - 249 | °C | - |
Température de la buse | 199 - 249 | °C | - |