Material datasheets available free. Online registration at: www.materialdatacenter.com
Zenite - LCP - Celanese
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Zenite" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...elby, North Carolina/USA, which had originally been planned for 2005, increasing its capacity by 40% to 8400t/a by 2004 (Table1). In 2004, DuPont took over the LCP sector from Eastman and now sells the former Titan product line under the name Zenite 5000. These materials round off DuPont’s LCP portfolio with grades showing extremely low warpage, high weld line strength and excellent impact resistance. Developing Materials Tailored to Demands Lead-free soldering, MID technology (MID: moulded i...
Kunststoffe international, 2005-11-21, High-performance Polymers: Metal Substitution and Miniaturisation
...e in a variety of applications. With LCP into the Future Liquid crystalline polymers (LCP) are characterised by very high toughness, heat resistance and low coefficient of thermal expansion. Among glass-fibre reinforced products, the Zenite LCP from DuPont can be found as a coil former and stator encapsulant in the torque engines of Soncboz SA. The mineral-filled E540i is “no typical LCP”, emphasises Ticona. The junior member of the Vectra family has a fine and – unusual for LCP – coloured sur...
Kunststoffe international, 2005-11-21, Liquid Crystal Polymers (LCP)
...e segment of the LCP market. Leading manufacturers are further refining their products and developing new ones to meet ever-increasing customer demands in this market segment for, e.g., extremely low ion content (Ticona: Vectra T840; DuPont: Zenite 7738), even higher heat resistance (Ticona: T and S series; DuPont 9000 series; Sumitomo: 6000 series) and greater isotropy in properties (Ticona: A460). Increasingly a well-balanced ratio of dielectric constant to loss factor with low coefficients of...
Kunststoffe international, 2005-11-21, Materials with Multiple Functions
...on density compared to conventional IC housings with improved heat conductivity and a decrease in the number of production steps (Fig.15) [2]. Also DuPont has announced the fact that its special liquid crystal polymer (Zenite LCP) for production of chip carriers according to the PSGA design method is being used by Siemens Dematic, Bruchsal/Germany. The dimensional stability and high temperature stability of the LCP are crucial conditions for the fact that accurate positioning of the contact pins...
Kunststoffe international, 2007-09-19, For High-End Applications
...irst Rynite parts are now being used in printers, lamp sockets and electrical/electronic components requiring a glow wire ignition temperature of 775°C according to IEC 60335. Two new grades, ZE55201 and ZE55801, have been added to the Zenite 5000 suite. ZE55201 is an ultra-low-warp material used to maintain flatness in elements such as connectors and chip card holders but also in larger components such as oven doors. ZE55801 is a palladium-doped, glass-fiber-reinforced LCP, which is highly suit...
Kunststoffe international, 2007-10-21, Liquid Crystal Polymers (LCPs)
... by Polyplastics, a joint venture run by Ticona and Daicel Chemical Industries. Sumitomo Chemical from Osaka produces a total of 5,000t/a in Harima and Niihama, Japan. Number three on the market is DuPont, which manufactures 3,500t/a (2005) of its Zenite brand in Chattanooga, Tennessee, USA. Further manufacturers are Solvay Advanced Polymers, Ueno and Toray. In terms of quantity, liquid crystal polymers play a subordinate role to engineering and even commodity plastics. But manufacturers such as...
Kunststoffe international, 2008-09-23, Set for Special Applications
.... In automotive applications polymeric materials are found which in the engine compartment area are progressively substituting metallic materials. These have direct contact with hot engine oil. The inherently nonflammable liquid crystalline plastic, Zenite, allows the low-cost production of light sockets in which it replaces ceramics. Hall B4, booth 4201 PolyOne Wide Range of Novelties By acquiring the GLS Corporation the PolyOne Corporation, Assesse, Belgium, has redoubled its commitment to the...
Kunststoffe international, 2010-09-24, Facilitating Technical Life
...al guidelines and meet up to the sector”s requirements – either through halogen-free flame retardants, such as for Celanex XFR PBT and Riteflex XFR TPC-ET, or through the inherent flame resistance of Fortron PPS, Vectra LCP or Zenite LCP. Typical fields of application are switches, plug connectors, housings, television sets and mobile phones. Hall 6, booth A07 and B07 DuPont Focus on Sustainability DuPont de Nemours GmbH, NeuIsenburg, Germany, is presenting advanced alternatives to metals for au...
Kunststoffe international, 2011-10-17, Liquid Crystal Polymers (LCP)
...et for LCPs is very well-defined. The largest manufacturers are Sumitomo Chemical Industry Ltd., Tokyo, Japan, with Sumikasuper, Solvay S.A., Brussels, Belgium, with Xydar and Celanese Corp. with Ticona GmbH, Sulzbach, Germany, with Vectra and Zenite and Polyplastics Co., Ltd. with Vectra. A wide variety of different LCP grades is offered for a multitude of applications in the electrical and electronics sectors as well as automotive, aircraft and aerospace industries. For 2013, a worldwide LCP d...
Kunststoffe international, 2013-08-19, Overcoming Complexity with Tailored Solutions
...for the electronics industry. Innovative materials and technologies are required. That is why industry partners Ticona GmbH, Sulzbach, Germany, and Delo Industrial Adhesives GmbH & Co. KGaA, Windach, Germany, are now combining Vectra and Zenite LCP (liquid crystal polymer) grades with specially tailored adhesives to create new solution packages that can withstand the high temperatures of reflow soldering. These combined packages are helping the electronics industry successfully miniaturize i...
Kunststoffe international, 2014-10-10, Liquid Crystal Polymers (LCP)
... in recent years. The major producers are Sumitomo Chemical Industry Ltd. in Tokyo, Japan, with their Sumikasuper brand; Solvay S.A. in Brussels, Belgium, with Xydar and Celanese Engineered Materials in Sulzbach, Germany, with their Vectra and Zenite brands, as well as Polyplastics Co., Ltd. in Tokyo, with Laperos. A wide range of different types of this high-performance plastic material is available to fit the needs of all major markets such as electrical and electronics, automotive and aerospa...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.