Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ULTEM™ Resin 2410EPR - Americas - PEI-GF40 - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for ULTEM™ Resin 2410EPR - Americas:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultem datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing.

UL Yellow Card Link E121562-221105
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 11 cm³/10min ISO 1133
Température 360 °C -
Charge 5 kg -
ASTM Data
Indice de fluidité, MFI 8.9 g/10min ASTM D 1238
Température 337 °C -
Charge 6.6 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 11000 MPa ISO 527
Contrainte d'écoulement 170 MPa ISO 527
Déformation au seuil d'écoulement 2 % ISO 527
Contrainte à la rupture 170 MPa ISO 527
Déformation à la rupture 2 % ISO 527
Module de flexion 9500 MPa ISO 178
Résistance au choc Charpy, +23°C 30 kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 35 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 10 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 10 kJ/m² ISO 179/1eA
Izod impact strength, +23°C, 4mm 30 kJ/m² ISO 180/1U
Izod impact strength, -30°C, 4mm 30 kJ/m² ISO 180/1U
Résistance au choc Izod (entaillé), +23°C, 4mm 10 kJ/m² ISO 180/1A
Résistance au choc Izod (entaillé), -30°C, 4mm 10 kJ/m² ISO 180/1A
Ball indentation hardness 165 MPa ISO 2039-1
ASTM Data
Module en traction 11100 MPa ASTM D 638
Module de traction d’élasticité 165 MPa ASTM D 638
Résistance de traction à la rupture 165 MPa ASTM D 638
Allongement d’élasticité 1.8 % ASTM D 638
Allongement à la rupture 1.8 % ASTM D 638
Module de flexion 10650 MPa ASTM D 790
Izod choc avec entaille, 1/8 in 82 J/m ASTM D 256
Résistance au choc Izod, 1/8 in 410 J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 197 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 206 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 214 °C ISO 306
Température de ramolliss. Vicat, 120°C/h 50N 215 °C ISO 306
Inflammabilité pr. épaisseur h V-0 class IEC 60695-11-10
Epaisseur de l'éprouvette 0.4 mm -
Conductivité thermique 0.3 W/(m K) DIN 52616
ASTM Data
DTUL à 66 psi 212 °C ASTM D 648
DTUL à 264 psi 204 °C ASTM D 648
Vicat température 223 °C ASTM D 1525
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.8 % Sim. to ISO 62
Absorption d'humidité 0.4 % Sim. to ISO 62
Masse volumique 1560 kg/m³ ISO 1183
Densité 1560 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 150 °C -
Pré-séchage - temps 4 - 6 h -
L'humidité de traitement ≤0.02 % -
Température de la matière fondue 350 - 400 °C -
Température du moule 135 - 165 °C -
Zone 1 330 - 400 °C -
Zone 2 340 - 400 °C -
Zone 3 345 - 400 °C -
Vitesse de rotation de vis 40 - 70 rpm -
Contre-pression 0.3 - 0.7 MPa -
Caractéristiques
Transformation
Moulage par injection
Disponibilité régionale
Amérique du nord
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.