Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ MP100 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ MP100:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit

Eastman Tritan™ MP100 is an amorphous copolyester that combines excellent clarity and toughness with outstanding heat and chemical resistance. Film and sheet manufactured from this new-generation copolyester can be thermoformed with a wide processing window that allows for product designs that reflect intricate detail.

Eastman Tritan™ MP100 copolyester is suitable for use with most forms of sterilization including radiation and ethylene oxide. It is NOT suitable for autoclave/steam sterilization. Eastman Tritan™ MP100 copolyester has been

formulated for use in medical film, sheet, and packaging applications.

Propriétés thermiquesValeurUnitéNorme du test
ASTM Data
coefficient de dilatation thermique, long. 88 E-6/K ASTM D 696
Température de transition vitreuse 110 °C ASTM E 1356
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Brillant 161 - ASTM D 2457
Haze 1 % ASTM D 1003
Lumière á Transmittance 92 % ASTM D 1003
Indice de réfraction 1.54 - ASTM D 542
Propriétés diversesValeurUnitéNorme du test
Absorption d’eau, 24hr 0.5 % ASTM D 570
Densité 1190 kg/m³ ASTM D 792
Propriétés mécaniques (Grades film)ValeurUnitéNorme du test
ISO Data
Résistance au déchirement pantalon, parallèle 11 N/mm ISO 6383-1
Résistance au déchirement pantalon, normal 11 N/mm ISO 6383-1
Epaisseur des eprouvettes 0.25 mm -
ASTM Data
Module en traction, long. 1460 MPa ASTM D 882
Module en traction, trav. 1380 MPa ASTM D 882
Module de traction d’élasticité, long. 41 MPa ASTM D 882
Module de traction d’élasticité, trav. 40 MPa ASTM D 882
Résistance de traction à la rupture, long. 59 MPa ASTM D 882
Résistance de traction à la rupture, trav. 52 MPa ASTM D 882
Allongement d’élasticité, long. 7 % ASTM D 882
Allongement d’élasticité, trav. 7 % ASTM D 882
Allongement à la rupture, long. 179 % ASTM D 882
Allongement à la rupture, trav. 203 % ASTM D 882
Epaisseur des eprouvettes 0.25 mm -
Caractéristiques
Transformation
Extrusion de films, Extrusion de plaques, Thermoformage
Propriétés spéciales
Stabilisé à la chaleur, Transparent, Stérilisable, Stérilisation par oxyde d'éthylène (EtO), Stérilisation par rayonnement gamma
Caractéristiques
Amorphe, Soudage à la chaleur, Copolymère
Résistance Chimique
Résistance chimique générale, Résistance au rayonnement
Applications
Médical, Emballage
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.