Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of SABIC® PP QR681K - PP - Saudi Basic Industries Corporation (SABIC)
Material Data Center offers the following functions for SABIC® PP QR681K:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
Informations produit
SABIC® PP QR681K is a new highly transparent random copolymer grade in the blow moulding product range. Impact, transparency, stiffness are well balanced and give you the opportunity to make weight optimized blow moulding products. This grade combines improved aesthetics of the finished articles with low temperature processability. Part aesthetics are not affected by the lower temperatures, providing for a broader operating window. High transparency, contact clarity and gloss will produce appealing blow moulded bottles. These properties, combined with a high heat deflection temperature, result in a wide variety of applications where the SABIC® PP QR681K can be used.
Application:
SABIC® PP QR681K is used for various blow moulding processes like Extrusion Blow Moulding and Injection (Stretch) Blow Moulding. SABIC® PP QR681K applications range from household to personal care products, but the material is also very suited for food packaging where a high heat distortion could be required.
Health, Safety and Food Contact regulations: Material Safety Data Sheets (MSDS) and Product Safety declarations are available on our Internet site
http://www.SABIC.com The product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/ medical applications.
Propriétés mécaniques | Valeur | Unité | Norme du test |
ISO Data |
Module en traction |
950 |
MPa |
ISO 527 |
Contrainte d'écoulement |
26 |
MPa |
ISO 527 |
Déformation au seuil d'écoulement |
13 |
% |
ISO 527 |
Résistance au choc Charpy (entaillé), +23°C |
8 |
kJ/m² |
ISO 179/1eA |
Propriétés thermiques | Valeur | Unité | Norme du test |
ISO Data |
Température de fléchissement s/chrg, 0.45 MPa |
65 |
°C |
ISO 75-1/-2 |
Caractéristiques
Propriétés spéciales
Transparent
Caractéristiques
Copolymère
Certifications
Contact alimentaire
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.