Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of SABIC® PP 622L - PP - Saudi Basic Industries Corporation (SABIC)
Material Data Center offers the following functions for SABIC® PP 622L:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
Informations produit
SABIC®PP 622L is a polypropylene random copolymer resin specifically designed for cast film applications. Products produced out of SABIC®PP 622L have a high clarity, excellent sealing performance and high puncture resistance. The molecular structure of this grade is tailored for high performance processing. SABIC®PP 622L contains anti-block and slip agent for low coefficient of friction. A grade without anti-block and slip agent is available as SABIC®PP 621P.
Applications: SABIC PP 622L is typically used in applications like food packaging, lamination film, stationary film, textile packaging, flower packaging, and hygiene packaging.
Health, Safety and Food Contact regulations: SABIC®PP 622L is compliant to food contact regulations. Material Safety Data Sheets (MSDS) and Product Safety declarations are available on our Internet site
http://www.SABIC.com
The product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/ medical applications. IMDS 80775790
Propriétés mécaniques | Valeur | Unité | Norme du test |
ISO Data |
Module en traction |
800 |
MPa |
ISO 527 |
Contrainte d'écoulement |
25 |
MPa |
ISO 527 |
Déformation au seuil d'écoulement |
13 |
% |
ISO 527 |
Propriétés thermiques | Valeur | Unité | Norme du test |
ISO Data |
Température de ramolliss. Vicat, A |
128 |
°C |
ISO 306 |
Température de ramolliss. Vicat, B |
63 |
°C |
ISO 306 |
Caractéristiques
Caractéristiques
Copolymère
Certifications
Contact alimentaire
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.