Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® LLDPE 726NE - (PE-LLD) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® LLDPE 726NE:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
SABIC® LLDPE 726NE is a butene linear low density polyethylene resin. This grade is designed to give blown films a relatively high stiffness for good machinability and a good overall balance of other performance properties, such as puncture resistance, impact strength and heat sealability. Application Typical applications for SABIC® LLDPE 726NE are shipping sacks, produce bags, can liners and carrier bags. SABIC® LLDPE 726NE has very good optical properties when blended with a LDPE (15-85%). Film properties Film of 50 ?m and BUR=2 has been produced on Kiefel IBC with 130 kg/h. Die size 200 mm, die gap 2,7 mm. This product is not intended for and must not be used in any pharmaceutical/medical applications.
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de ramolliss. Vicat, A 110 °C ISO 306
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Haze 12 % ASTM D 1003
Propriétés mécaniques (Grades film)ValeurUnitéNorme du test
ISO Data
Module en traction, parallèle 220 MPa ISO 527-3
Module en traction, perpend. 240 MPa ISO 527-3
Contrainte au seuil, parallèle 13 MPa ISO 527-3
Contrainte au seuil, normal 14 MPa ISO 527-3
Contrainte à la rupture, parallèle 45 MPa ISO 527-3
Contrainte à la rupture, perpend. 35 MPa ISO 527-3
Résistance au déchirement pantalon, parallèle 20 N/mm ISO 6383-1
Résistance au déchirement pantalon, normal 130 N/mm ISO 6383-1
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.