Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of RADISTRONG AROMA RV500RKC2 306 BK - (PA66+PA*)-GF50 - RadiciGroup High Performance Polymers

Material Data Center offers the following functions for RADISTRONG AROMA RV500RKC2 306 BK:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Radistrong datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Special PA 50% glass fibre reinforced, high flow injection moulding grade. Heat stabilized. Drinking water and food contact. Black colour.

General purpose metal replacement product  with good resistance to hydrolysis, enhanced mechanical properties after moisture pick-up. Specifically intended for use in applications in civil and industrial water management as well as appliances and consumer goods. Suitable for parts requiring very high stiffness and high mechanical resistance along with high surface quality and superior gloss.
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Retrait au moulage, parallèle 0.2 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.6 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 17500 / 16300 MPa ISO 527
Contrainte à la rupture 235 / 190 MPa ISO 527
Déformation à la rupture 2.4 / 2.8 % ISO 527
Résistance au choc Charpy, +23°C 95 / 95 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 15 / 15 kJ/m² ISO 179/1eA
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 256 / * °C ISO 11357-1/-3
Propriétés diversessec / condUnitéNorme du test
Absorption d'humidité 1.1 / * % Sim. to ISO 62
Masse volumique 1590 / - kg/m³ ISO 1183
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Grains, Noir
Additifs
Agent de démoulage
Propriétés spéciales
Stabilisé à la chaleur
Caractéristiques
High Gloss
Résistance Chimique
Stabilité hydrolytique
Certifications
Contact alimentaire, Contact avec l'eau potable
Applications
General Purpose
Disponibilité régionale
Autres informations
Moulages par injection
The material is delivered in moisture-proof packaging ready for processing. Maximum recommended water content for best processing is 0.15%. Typical conditions with a desiccant drier: temperature 80 ° C, dew point -20 ° C or below, time 2-4 h or more. Special care must be taken to avoid moisture absorption and contamination with other polymers when adding regrind material. Colour variation and mechanical properties reduction may occur and should always be carefully monitored.

Injection Molding Processing Parameters
Melt Temperature Mold Temperature Injection Speed
280 - 300°C 80 - 100°C medium-high
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.