Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL™ Resin NHP5054 - Europe - (PPE+PS)-GF20 - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL™ Resin NHP5054 - Europe:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
NORYL™ NHP5054 resin is a 20% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of V0 at 0.75mm for thin-wall molding capability. NORYL NHP5054 is based on a unique co-polymer technology and exhibits good dimensional stability, high heat resistance, strong electrical performance, and very low specific gravity. It is an excellent candidate for electrical vehicle (EV) battery housings, automotive under-the-hood enclosures and components where thin-wall FR, modulus retention, and high heat resistance are required.

UL Yellow Card Link E207780-101793092
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 22 cm³/10min ISO 1133
Température 280 °C -
Charge 10 kg -
ASTM Data
Indice de fluidité, MFI 24 g/10min ASTM D 1238
Température 250 °C -
Charge 10 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 7300 MPa ISO 527
Contrainte à la rupture 110 MPa ISO 527
Déformation à la rupture 2.4 % ISO 527
Module de flexion 6000 MPa ISO 178
Résistance au choc Charpy, +23°C 35 kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 36 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 9 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 8 kJ/m² ISO 179/1eA
Ball indentation hardness 215 MPa ISO 2039-1
ASTM Data
Module de traction d’élasticité 120 MPa ASTM D 638
Allongement à la rupture 2.5 % ASTM D 638
Izod choc avec entaille, 1/8 in 100 J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 115 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 122 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 128 °C ISO 306
Température de ramolliss. Vicat, 120°C/h 50N 130 °C ISO 306
Inflammabilité pr. épaisseur h V-0 class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Ignition Temperature (GWIT) 775 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Glow Wire Ignition Temperature (GWIT) 800 °C IEC 60695-2-13
GWIT - thickness tested (2) 2 mm -
GWIT - thickness tested (3) 3 mm -
Propriétés diversesValeurUnitéNorme du test
Absorption d'humidité 0.24 % Sim. to ISO 62
Masse volumique 1270 kg/m³ ISO 1183
Densité 1300 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 105 - 110 °C -
Pré-séchage - temps 3 - 4 h -
L'humidité de traitement ≤0.02 % -
Température de la matière fondue 280 - 310 °C -
Température du moule 75 - 105 °C -
Zone 1 250 - 300 °C -
Zone 2 260 - 305 °C -
Zone 3 270 - 310 °C -
Vitesse de rotation de vis 20 - 100 rpm -
Contre-pression 0.3 - 0.7 MPa -
Caractéristiques
Transformation
Moulage par injection
Additifs
Agent ignifugeant
Propriétés spéciales
Ignifugé
Applications
Automobile
Disponibilité régionale
Europe
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.