Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Monprene® RG-10150 - TPE - Teknor Apex Co.

Material Data Center offers the following functions for Monprene® RG-10150:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Monprene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Preliminary Data

The Monprene RG-10100 series is a group of high performance thermoplastic elastomers specifically designed for regulated applications including food contact, toys, and children's products. Monprene RG-10150 is a low density, medium hardness grade that complies with various US FDA and European regulations and directives for food contact and toy safety and is suitable for injection molding.

Adheres to PP

PropertyValueUnitStandard
Tensile Stress at 100% (across flow)0.87MPaISO 37
Tensile Stress at break (across flow)6.8MPaISO 37
Tensile Strain at Break (across flow840%ISO 37
Tear Strength (across flow)11kN/mISO 34-1
Apparent Viscosity (200 °C, 206 1/s)226PasASTM D3835
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Indice de fluidité, MFI 4 g/10min ASTM D 1238
Température 200 °C -
Charge 5 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Déformation rémanente en compression à 70 °C, 24h 25 % ISO 815
Résistance à la déchirure 19 kN/m ISO 34-1
Dureté Shore A 50 - ISO 7619-1
Propriétés diversesValeurUnitéNorme du test
Densité 888 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 65 °C -
Pré-séchage - temps 2 - 4 h -
Température de la matière fondue 182 - 227 °C -
Température du moule 27 - 49 °C -
Zone 1 160 - 177 °C -
Zone 2 182 - 204 °C -
Zone 3 193 - 216 °C -
Température de la buse 182 - 227 °C -
Vitesse de rotation de vis 50 - 100 rpm -
Contre-pression 0.172 - 0.689 MPa -
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Additifs
Lubrifiant
Propriétés spéciales
Translucent
Caractéristiques
Bonne adhérence
Certifications
Contact alimentaire, FDA 21 CFR approbation
Applications
Emballage
Disponibilité régionale
Amérique du nord, Europe, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.