Caractéristiques des transformations/physiques | Valeur | Unité | Norme du test |
ISO Data |
Indice de fluidité à chaud en volume, MVR |
18 |
cm³/10min |
ISO 1133 |
Température |
190 |
°C |
- |
Charge |
2.16 |
kg |
- |
Other Standards[S] |
Retrait au moulage, parallèle |
3.0 |
% |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés mécaniques | Valeur | Unité | Norme du test |
ISO Data |
Dureté Shore A |
88 |
- |
ISO 7619-1 |
Other Standards[S] |
Module de flexion, 23°C |
27 |
MPa |
ISO 6721-1 |
Module de flexion |
72 |
MPa |
ISO 6721-1 |
Module de flexion - Température |
60 |
°C |
- |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés thermiques | Valeur | Unité | Norme du test |
ISO Data |
Température de fusion, 10°C/min |
160 |
°C |
ISO 11357-1/-3 |
Température de ramolliss. Vicat, A |
90 |
°C |
ISO 306 |
Other Standards[S] |
Température de transition vitreuse, 10°C/min |
-13.6 |
°C |
ISO 6721-1 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés diverses | Valeur | Unité | Norme du test |
Masse volumique |
1200 |
kg/m³ |
ISO 1183 |
Bulk density |
457 |
kg/m³ |
- |
3D Data | Valeur | Unité | Norme du test |
Other Standards[S] |
Résistance à la traction, flat |
20[1] |
MPa |
DIN 53504 |
Résistance à la traction, upright |
15[2] |
MPa |
DIN 53504 |
Déformation à la rupture, flat |
520[1] |
% |
DIN 53504 |
Déformation à la rupture, upright |
500[2] |
% |
DIN 53504 |
1: | XY-direction | 2: | ZX-direction | S: | These properties are reported by the producer according standards that are different to our defaults. |
Caractéristiques
Transformation
Additive Manufacturing, Frittage laser
Conditionnement
Poudre, Blanc
Applications
Sport
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com