Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEXAN™ Copolymer EXL9330 - Asia - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for LEXAN™ Copolymer EXL9330 - Asia:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lexan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
EXL9330 is an opaque (PC)- siloxane copolymer resin that offers extreme low temperature (-60 C) ductility in combination with excellent processability. This UV stabilized, medium flow resin features UL f1/V-0/5VA rating with non-chlorinated, non-brominated flame retardant agents for wide range of colors. EXL9330 is an excellent candidate for a broad range of applications such as mobile phones, tablets, industrial housings, electric circuit protection, personal safety helmets, electric vehicle supply equipment (EVSE) housings and connectors.

UL Yellow Card Link E207780-228378
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 9 cm³/10min ISO 1133
Température 300 °C -
Charge 1.2 kg -
ASTM Data
Indice de fluidité, MFI 10 g/10min ASTM D 1238
Température 300 °C -
Charge 1.2 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 2100 MPa ISO 527
Contrainte d'écoulement 55 MPa ISO 527
Déformation au seuil d'écoulement 6 % ISO 527
Contrainte à la rupture 60 MPa ISO 527
Déformation à la rupture 50 % ISO 527
Module de flexion 2200 MPa ISO 178
Résistance au choc Charpy, +23°C, 3mm N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C, 3mm N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C, 3mm 75 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C, 3mm 60 kJ/m² ISO 179/1eA
Résistance au choc Izod, +23°C N kJ/m² ISO 180/1U
Résistance au choc Izod (entaillé), +23°C, 3mm 70 kJ/m² ISO 180/1A
Résistance au choc Izod (entaillé), -30°C, 3mm 55 kJ/m² ISO 180/1A
Ball indentation hardness 90 MPa ISO 2039-1
ASTM Data
Module en traction 2100 MPa ASTM D 638
Module de traction d’élasticité 58 MPa ASTM D 638
Résistance de traction à la rupture 61 MPa ASTM D 638
Allongement d’élasticité 6 % ASTM D 638
Allongement à la rupture 130 % ASTM D 638
Module de flexion 2060 MPa ASTM D 790
Izod choc avec entaille, 1/8 in 801 J/m ASTM D 256
Izod choc avec entaille, 1/4 in 640 J/m ASTM D 256
Izod choc avec entaille, bas température 678 J/m ASTM D 256
Température -30 °C -
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de ramolliss. Vicat, B 140 °C ISO 306
Température de ramolliss. Vicat, 120°C/h 50N 142 °C ISO 306
Inflammabilité ep. nom. 1.5 mm V-0 class IEC 60695-11-10
Epaisseur de l'éprouvette 1.5 mm -
Inflammabilité pr. épaisseur h V-1 class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 mm -
Inflammabilité 5V pr. épaisseur h 5VB class IEC 60695-11-20
Epaisseur de l'éprouvette 2.5 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Ignition Temperature (GWIT) 825 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Glow Wire Ignition Temperature (GWIT) 825 °C IEC 60695-2-13
GWIT - thickness tested (2) 2 mm -
Glow Wire Ignition Temperature (GWIT) 825 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM Data
DTUL à 66 psi 134 °C ASTM D 648
DTUL à 264 psi 120 °C ASTM D 648
Vicat température 142 °C ASTM D 1525
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 1MHz 2.7 - IEC 62631-2-1
Facteur de pertes, 1MHz 85 E-4 IEC 62631-2-1
Résistivité transversale >1E13 Ohm*m IEC 62631-3-1
Résistivité superficielle >1E15 Ohm IEC 62631-3-2
Indice de résistance au cheminement 225 - IEC 60112
ASTM Data
Rigidité diélectrique, peu de temps 17 kV/mm ASTM D 149
Facteur de dissipation diélectrique, 60 Hz 0.0024 - ASTM D 150
Facteur de dissipation diélectrique, 1 MHz 0.0085 - ASTM D 150
Constante diélectrique, 60 Hz 2.95 - ASTM D 150
Constante diélectrique, 1 MHz 2.9 - ASTM D 150
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.35 % Sim. to ISO 62
Absorption d'humidité 0.15 % Sim. to ISO 62
Masse volumique 1190 kg/m³ ISO 1183
Densité 1180 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 120 °C -
Pré-séchage - temps 3 - 4 h -
L'humidité de traitement ≤0.02 % -
Température de la matière fondue 255 - 315 °C -
Température du moule 70 - 95 °C -
Zone 1 235 - 295 °C -
Zone 2 245 - 305 °C -
Zone 3 255 - 315 °C -
Vitesse de rotation de vis 40 - 70 rpm -
Contre-pression 0.3 - 0.7 MPa -
Caractéristiques
Transformation
Moulage par injection
Additifs
Agent ignifugeant
Propriétés spéciales
Ignifugé
Applications
Automobile
Disponibilité régionale
Asia Pacific
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.