Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Hycar" in Material Data Center leads to the following information:

Tradename: Hycar
Family: ACM
Producer: The Lubrizol Corporation
1 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Kunststoffe international, 2005-11-21, Impact Modification Of Thermosets
...ter this, the hardener was added, degassed in a vacuum and cured in line with the usual specifications at elevated temperature. For comparison, a specimen was modified with 10 % by wt. of a carboxyl-functionalized acrylonitrile butadiene copolymer (Hycar CTBN from BF Goodrich). Fracture-mechanical Properties The fracture toughness and fracture energy are a good measure of the brittleness of a material. The main emphasis of the study was therefore on determining these values. The fracture tough...


Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.