Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Grivory HT2V-5H black 9205 - PA6T/66-GF50 - EMS-GRIVORY | a unit of EMS-CHEMIE AG

Material Data Center offers the following functions for Grivory HT2V-5H black 9205:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Grivory datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Product-nomenclature: ISO 16396-PA6T/66,GF50,M1H,C14-190

 

Co Polyamide

Partially aromatic Polyamide

Product Attributes

  Improved heat resistance, Improved UV resistance (outdoor use)

Markets

  Automotive
  Air intake sytems, Automotive electr. and electronics, lighting, Fuel systems,
Powertrain and Chassis, Interior, Exterior
  Electricals & Electronics
  Electrical appliances, Electrical equipment
  Industry & Consumer goods
  Housewares, Hydraulics & Pneumatics, Mechanical Engineering, Power transmission, Sports & Leisure,
Tools & Accessories
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Retrait au moulage, parallèle 0.1 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.7 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 17500 / 17000 MPa ISO 527
Contrainte à la rupture 250 / 225 MPa ISO 527
Déformation à la rupture 2 / 2 % ISO 527
Résistance au choc Charpy, +23°C 75 / 75 kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 60 / 60 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 11 / 11 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 11 / 10 kJ/m² ISO 179/1eA
Dureté Shore D 91 / * - ISO 7619-1
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 310 / * °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 280 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 8.00 MPa 230 / * °C ISO 75-1/-2
Coeffic. de dilatation therm. linéique, parallèle 10 / * E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 55 / * E-6/K ISO 11359-1/-2
Inflammabilité pr. épaisseur h HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 / * mm -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Résistivité transversale 1E10 / 1E10 Ohm*m IEC 62631-3-1
Résistivité superficielle * / 1E12 Ohm IEC 62631-3-2
Rigidité diélectrique 38 / 38 kV/mm IEC 60243-1
Indice de résistance au cheminement - / 600 - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 3.5 / * % Sim. to ISO 62
Absorption d'humidité 1.2 / * % Sim. to ISO 62
Masse volumique 1620 / - kg/m³ ISO 1183
Fonctions
Viscosité / Vitesse de cisaillement , Grivory HT2V-5H black 9205, PA6T/66-GF50, EMS-GRIVORY
Contrainte de cisaillement / Vit. de cisaillement , Grivory HT2V-5H black 9205, PA6T/66-GF50, EMS-GRIVORY
Module de cisaillement dynamique / Température , Grivory HT2V-5H black 9205 (sec), PA6T/66-GF50, EMS-GRIVORY
Module de cisaillement dynamique / Température , Grivory HT2V-5H black 9205 (cond.), PA6T/66-GF50, EMS-GRIVORY
Contrainte / Déformation , Grivory HT2V-5H black 9205 (sec), PA6T/66-GF50, EMS-GRIVORY
Contrainte / Déformation , Grivory HT2V-5H black 9205 (cond.), PA6T/66-GF50, EMS-GRIVORY
Module sécant / Déformation , Grivory HT2V-5H black 9205 (sec), PA6T/66-GF50, EMS-GRIVORY
Module sécant / Déformation , Grivory HT2V-5H black 9205 (cond.), PA6T/66-GF50, EMS-GRIVORY
Contrainte / Déformation (isochrone) 23°C, Grivory HT2V-5H black 9205 (cond.), PA6T/66-GF50, EMS-GRIVORY
Module de fluage / Temps 23°C, Grivory HT2V-5H black 9205 (cond.), PA6T/66-GF50, EMS-GRIVORY
Courbe de fluage 23°C, Grivory HT2V-5H black 9205 (cond.), PA6T/66-GF50, EMS-GRIVORY
Contrainte / Déformation (isochrone) 80°C, Grivory HT2V-5H black 9205 (sec), PA6T/66-GF50, EMS-GRIVORY
Module de fluage / Temps 80°C, Grivory HT2V-5H black 9205 (sec), PA6T/66-GF50, EMS-GRIVORY
Courbe de fluage 80°C, Grivory HT2V-5H black 9205 (sec), PA6T/66-GF50, EMS-GRIVORY
Volume spécifique (pvT) , Grivory HT2V-5H black 9205, PA6T/66-GF50, EMS-GRIVORY
Module de traction / Température , Grivory HT2V-5H black 9205 (sec), PA6T/66-GF50, EMS-GRIVORY
Module de traction / Température , Grivory HT2V-5H black 9205 (cond.), PA6T/66-GF50, EMS-GRIVORY
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Grains, Noir
Propriétés spéciales
Stabilisé aux intempéries, Stabilisé à la chaleur
Caractéristiques
Copolymère
Applications
Automobile, Électrotechnique et électrique, Sport
Disponibilité régionale
Résistance Chimique
Acides
Acide acétique (masse en 5%) (23°C)
Acide citrique (masse en 10%) (23°C)
Acide lactique (masse en 10%) (23°C)
Acide chlorhydrique (masse en 36%) (23°C)
Acide nitrique (masse en 40%) (23°C)
Acide sulfurique (masse en 38%) (23°C)
Acide sulfurique (masse en 5%) (23°C)
Acide chromique (masse en 40%) (23°C)
Bases
Hydroxyde de soude (masse en 35%) (23°C)
Hydroxyde de soude (masse en 1%) (23°C)
Hydroxyde d'ammoniaque (masse en 10%) (23°C)
Alcool
Isopropanol (23°C)
Méthanol (23°C)
Ethanol (23°C)
Hydrocarbures
n-Hexane (23°C)
Toluene (23°C)
iso-Octane (23°C)
Cetones
Acetone (23°C)
Ethers
Diethyl ether (23°C)
Huiles minérales
Huile moteur multigrade SAE 10W40 (23°C)
Huile moteur multigrade SAE 10W40 (130°C)
Huile engrenage hypoide SAE 80/90 (130°C)
Huile d'isolation (23°C)
Carburants standards
ISO 1817 Liquide 1 (60°C)
ISO 1817 Liquide 2 (60°C)
ISO 1817 Liquide 3 (60°C)
ISO 1817 Liquide 4 (60°C)
Carburant stand. sans alcool (de pref. ISO 1817 liquide C) (23°C)
Carburant stand. avec alcool (de pref. ISO 1817 Liquid 4) (23°C)
Gasoil (pref. ISO 1817 liquide F) (23°C)
Gasoil (pref. ISO 1817 liquide F) (90°C)
Gasoil (pref. ISO 1817 liquide F) (>90°C)
Selts
Chlorure de sodium (masse en 10%) (23°C)
Hypochlorite de soude (masse en 10%) (23°C)
Carbonate de soude (masse en 20%) (23°C)
Carbonate de soude (masse en 2%) (23°C)
Chlorure de zinc (masse en 50%) (23°C)
Autres
Acétate d'éthyle (23°C)
Peroxyde d'hydrogene (23°C)
Liquide de frein DOT N° 4 (130°C)
Ethylene glycol (108°C)
1% nonylphenoxy-polyethyleneoxy dans l'eau (23°C)
50% Acide oléique + 50% d'huile d'olive (23°C)
L'eau (23°C)
L'eau déionisée (90°C)
Phénol (masse en 5%) (23°C)
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.