Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Grilon F 40 NL natural 6041 - PA6 - EMS-GRIVORY | a unit of EMS-CHEMIE AG

Material Data Center offers the following functions for Grilon F 40 NL natural 6041:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Grilon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Product nomenclature: ISO 16396-PA6,,FS,S27-030N

 

Product Attributes

  High viscosity, Highly transparent, Barrier material, Nucleated

Markets

  Packaging
  Non oriented film, Oriented film, Paper coating, Tubes

Approvals

  Food Contact
  EU Requirements, FDA
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 25 / * cm³/10min ISO 1133
Température 275 / * °C -
Charge 5 / * kg -
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction - / 750 MPa ISO 527
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 222 / * °C ISO 11357-1/-3
Propriétés optiquessec / condUnitéNorme du test
ISO Data
Brillance, 60° 100 / * - ISO 2813
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 9 / * % Sim. to ISO 62
Absorption d'humidité 3 / * % Sim. to ISO 62
Masse volumique 1140 / - kg/m³ ISO 1183
Propriétés mécaniques (Grades film)sec / condUnitéNorme du test
ISO Data
Contrainte au seuil, parallèle 35 / * MPa ISO 527-3
Contrainte au seuil, perpend. 30 / * MPa ISO 527-3
Déformation au seuil, parallèle 15 / * % ISO 527-3
Déformation au seuil, perpend. 15 / * % ISO 527-3
Déformation maximale, parallèle 700 / * % ISO 527-3
Déformation maximale, perpend. 700 / * % ISO 527-3
Résistance à la déchirure Elmendorf, parallèle 10 / * N ISO 6383-2
Résistance à la déchirure Elmendorf, perpend. 10 / * N ISO 6383-2
Résistance au déchirement pantalon, parallèle 30 / * N/mm ISO 6383-1
Résistance au déchirement pantalon, perpend. 30 / * N/mm ISO 6383-1
Coefficient de friction dynamique 0.25 / * - ISO 8295
Perméabilité à la vapeur d'eau, 23°C/85%r.h. 15 / * g/(m²*d) ISO 15106-1/-2
Perméabilité à l'oxygène, 23°C/0%r.h. 25 / * cm³/(m²*d*bar) ISO 15105-1/-2
Perméabilité à l'oxygène, 23°C/85%r.h. 50 / * cm³/(m²*d*bar) ISO 15105-1/-2
Perméabilité au gaz carbonique, 23°C/0%r.h. 80 / * cm³/(m²*d*bar) ISO 15105-1/-2
Perméabilité au gaz carbonique, 23°C/85%r.h. 250 / * cm³/(m²*d*bar) ISO 15105-1/-2
Fonctions
Viscosité / Vitesse de cisaillement , Grilon F 40 NL natural 6041, PA6, EMS-GRIVORY
Contrainte de cisaillement / Vit. de cisaillement , Grilon F 40 NL natural 6041, PA6, EMS-GRIVORY
Contrainte / Déformation (Grade film) , Grilon F 40 NL natural 6041 (cond.), PA6, EMS-GRIVORY
Caractéristiques
Transformation
Extrusion de films, Extrusion (autres), Enduction
Conditionnement
Grains, Couleurs naturelles
Additifs
Lubrifiant
Propriétés spéciales
Transparent
Caractéristiques
Propriétés barrière, Nuclée
Certifications
Contact alimentaire, FDA 21 CFR approbation
Applications
Emballage
Disponibilité régionale
Résistance Chimique
Acides
Acide acétique (masse en 5%) (23°C)
Acide citrique (masse en 10%) (23°C)
Acide lactique (masse en 10%) (23°C)
Acide chlorhydrique (masse en 36%) (23°C)
Acide nitrique (masse en 40%) (23°C)
Acide sulfurique (masse en 38%) (23°C)
Acide sulfurique (masse en 5%) (23°C)
Acide chromique (masse en 40%) (23°C)
Bases
Hydroxyde de soude (masse en 35%) (23°C)
Hydroxyde de soude (masse en 1%) (23°C)
Hydroxyde d'ammoniaque (masse en 10%) (23°C)
Alcool
Isopropanol (23°C)
Méthanol (23°C)
Ethanol (23°C)
Hydrocarbures
n-Hexane (23°C)
Toluene (23°C)
iso-Octane (23°C)
Cetones
Acetone (23°C)
Ethers
Diethyl ether (23°C)
Huiles minérales
Huile moteur multigrade SAE 10W40 (23°C)
Huile moteur multigrade SAE 10W40 (130°C)
Huile engrenage hypoide SAE 80/90 (130°C)
Huile d'isolation (23°C)
Carburants standards
ISO 1817 Liquide 1 (60°C)
ISO 1817 Liquide 2 (60°C)
ISO 1817 Liquide 3 (60°C)
ISO 1817 Liquide 4 (60°C)
Carburant stand. sans alcool (de pref. ISO 1817 liquide C) (23°C)
Carburant stand. avec alcool (de pref. ISO 1817 Liquid 4) (23°C)
Gasoil (pref. ISO 1817 liquide F) (23°C)
Gasoil (pref. ISO 1817 liquide F) (90°C)
Gasoil (pref. ISO 1817 liquide F) (>90°C)
Selts
Chlorure de sodium (masse en 10%) (23°C)
Hypochlorite de soude (masse en 10%) (23°C)
Carbonate de soude (masse en 20%) (23°C)
Carbonate de soude (masse en 2%) (23°C)
Chlorure de zinc (masse en 50%) (23°C)
Autres
Acétate d'éthyle (23°C)
Peroxyde d'hydrogene (23°C)
Liquide de frein DOT N° 4 (130°C)
Ethylene glycol (108°C)
1% nonylphenoxy-polyethyleneoxy dans l'eau (23°C)
50% Acide oléique + 50% d'huile d'olive (23°C)
L'eau (23°C)
L'eau déionisée (90°C)
Phénol (masse en 5%) (23°C)
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.