Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Delrin® 100ST BK602 - POM - DuPont Engineering Polymers

Material Data Center offers the following functions for Delrin® 100ST BK602:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Delrin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Common features of Delrin® acetal resins include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents, and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating, and available in a variety of colors and speciality grades.

Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics, and consumer goods industries.

Delrin® 100ST is a super-toughened, high viscosity acetal homopolymer grade with superior impact resistance.  It is designed for highly stressed parts where outstanding toughness is essential.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 1.8 cm³/10min ISO 1133
Température 190 °C -
Charge 2.16 kg -
Retrait au moulage, parallèle 0.8 % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.1 % ISO 294-4, 2577
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 1400 MPa ISO 527
Contrainte d'écoulement 40 MPa ISO 527
Déformation au seuil d'écoulement 30 % ISO 527
Déformation nominale à la rupture >50 % ISO 527
Résistance au choc Charpy, +23°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 80 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 14 kJ/m² ISO 179/1eA
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 178 °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 60 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 102 °C ISO 75-1/-2
Coeffic. de dilatation therm. linéique, parallèle 120 E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 120 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.5 mm -
Yellow Card disponible oui - -
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1340 kg/m³ ISO 1183
Fonctions
Module de cisaillement dynamique / Température , Delrin® 100ST BK602, POM, DuPont
Contrainte / Déformation , Delrin® 100ST BK602, POM, DuPont
Module sécant / Déformation , Delrin® 100ST BK602, POM, DuPont
Caractéristiques
Transformation
Moulage par injection, Extrusion de profilés, Extrusion de plaques, Extrusion (autres)
Conditionnement
Granulés, Noir
Additifs
Lubrifiant, Agent de démoulage
Propriétés spéciales
Modifié choc
Caractéristiques
Homopolymère
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.