Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Celazole® PBI U-60 - PBI - PBI Performance Products, Inc.

Material Data Center offers the following functions for Celazole® PBI U-60:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Celazole datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Propriétés mécaniquesValeurUnitéNorme du test
ASTM Data
Module en traction 5900 MPa ASTM D 638
Module de traction 160 MPa ASTM D 638
Module à la compression 5900 MPa ASTM D 695
Module de flexion 6500 MPa ASTM D 790
Résistance à la flexion 220 MPa ASTM D 790
Dureté Rockwell M 125 - ASTM D 785
Dureté D Shore 95 - ASTM D 2240
Izod choc avec entaille, 1/8 in 30 J/m ASTM D 256
Résistance au choc Izod, 1/8 in 590 J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ASTM Data
DTUL à 264 psi 435 °C ASTM D 648
Indice limite d’oxygène 58 % ASTM D 2863
Propriétés électriquesValeurUnitéNorme du test
ASTM Data
Rigidité diélectrique, peu de temps 23 kV/mm ASTM D 149
Résistance volumique >1E15 Ohm*cm ASTM D 257
Résistance à l’arc 185 s ASTM D 495
Propriétés diversesValeurUnitéNorme du test
Absorption d’eau, 24hr 0.4 % ASTM D 570
Densité 1300 kg/m³ ASTM D 792
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Propriétés spéciales
Ignifugé, Stabilisé à la chaleur
Caractéristiques
Résistance à la fatigue, Stabilité thermique, Grade tribologique
Résistance Chimique
Résistance chimique générale, Stabilité hydrolytique
Applications
Avions et aéronautique, Électrotechnique et électrique
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.