Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ALFATER XL D40E 2GP0000 - TPV - MOCOM Compounds GmbH & Co. KG

Material Data Center offers the following functions for ALFATER XL D40E 2GP0000:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Alfater datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Base PolymerThermoplastic Vulcanisate (PP+EPDM)
Colourblack,natural color
Service Temperaturemax. range (depending on load, geometry, etc.) -40-125 °C
Special Featureshigh viscosity,good weathering resistance,good chemical resistance,good ozone reistance,good hot air resistance,good hydrolysis resistant
Market SegmentAutomotive,building and construction,Machinery,electrical and electronic,Furniture
Application Areaextruded parts,blow moulded parts,coextrusion
Typical Applicationsprofile,seals,sealing lip,conduit,tubes,cable guides,cable jacketing,bellows,air duct,2K components
Adhesion toPolypropylene Homopolymer,Polypropylene Copolymer,Polyethylene,Thermoplastic Vulcanisate (PP+EPDM),Thermoplastic Olefin Elastomer,Thermoplastic Elastomer general
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Résistance à la déchirure 71 kN/m ISO 34-1
Dureté Shore D 40 - ISO 7619-1
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Coeffic. de dilatation therm. linéique, parallèle 9.1 E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 14.1 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.5 mm -
Yellow Card disponible oui - -
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Indice de résistance au cheminement 600 - IEC 60112
Propriétés diversesValeurUnitéNorme du test
Masse volumique 950 kg/m³ ISO 1183
Fonctions
Viscosité / Vitesse de cisaillement , ALFATER XL D40E 2GP0000, TPV, MOCOM
Contrainte de cisaillement / Vit. de cisaillement , ALFATER XL D40E 2GP0000, TPV, MOCOM
Module de cisaillement dynamique / Température , ALFATER XL D40E 2GP0000, TPV, MOCOM
Contrainte / Déformation (TPE) , ALFATER XL D40E 2GP0000, TPV, MOCOM
Volume spécifique (pvT) , ALFATER XL D40E 2GP0000, TPV, MOCOM
Caractéristiques
Transformation
Moulage par injection, Extrusion (autres), Soufflage
Propriétés spéciales
Stabilisé aux intempéries
Disponibilité régionale
Autres informations
Moulages par injection
Pre-Drying Conditionsin a dry air (dessiccant) dryer 70-80 °C
for 2-4 h
max. moisture content <0,10 %
Processing Extrusionmelt temperature 190-230 °C
die temperature 190-220 °C
Storagedry, protected from light
tightly sealed
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.