Caracteristicas de procesamiento y fisicas | Valor | Unidades | Método de ensayo |
Other Standards[S] |
Contracción posterior al moldeo, paralelo |
0.1 |
% |
DIN 16901 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propiedades mecánicas | Valor | Unidades | Método de ensayo |
ISO Data |
Módulo de tracción |
15000 |
MPa |
ISO 527 |
Esfuerzo de tracción |
170 |
MPa |
ISO 527 |
Resistencia al impacto Charpy, +23°C |
47 |
kJ/m² |
ISO 179/1eU |
Propiedades térmicas | Valor | Unidades | Método de ensayo |
ISO Data |
Estabilidad al calor, 1.80 MPa |
240 |
°C |
ISO 75-1/-2 |
Other Standards[S] |
Coef.de expansión térmica lineal, paralelo |
4 |
E-6/K |
DIN 53752 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propiedades eléctricas | Valor | Unidades | Método de ensayo |
ISO Data |
Resistividad superficial específica |
100 |
Ohm |
IEC 62631-3-2 |
Otras propiedades | Valor | Unidades | Método de ensayo |
Densidad |
1400 |
kg/m³ |
ISO 1183 |
Recomendación para procesamiento Extrusión | Valor | Unidades | Método de ensayo |
Temperatura de pre-secado |
130 |
°C |
- |
Tiempo de pre-secado |
6 - 8 |
h |
- |
Temperatura de la masa |
280 |
°C |
- |
Zona 1 |
260 - 300 |
°C |
- |
Zona 2 |
260 - 300 |
°C |
- |
Zona 3 |
260 - 300 |
°C |
- |
Temperatura de boquilla |
250 - 290 |
°C |
- |
Características
Procesamiento y forma de entrega
Otros tipos de extrusión, Additive Manufacturing
Forma de suministro
Sémola, Negro, Color natural
Características especiales
Estable contra el calor
Applicaciones
Automotriz, Filament for 3D Printing
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com