Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Delrin® 100ALE NC010 - POM-Z - DuPont Engineering Polymers

Material Data Center offers the following functions for Delrin® 100ALE NC010:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Delrin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Common features of Delrin® acetal resins include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents, and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating, and available in a variety of colors and speciality grades.

Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics, and consumer goods industries.

Delrin® 100ALE is a high viscosity acetal homopolymer with very low VOC emissions for applications in automotive interiors. It contains an advanced system of lubrication designed for low wear, low friction, and low noise against metals and plastics. 
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Contracción posterior al moldeo, paralelo 2.0 % ISO 294-4, 2577
Contracción posterior al moldeo, normal 1.7 % ISO 294-4, 2577
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 3000 MPa ISO 527
Esfuerzo de fluencia 70 MPa ISO 527
Alarg. en límite elástico 18 % ISO 527
Alarg. nominal a rotura 40 % ISO 527
Resistencia al impacto Charpy, +23°C N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C 200 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 10.5 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 8 kJ/m² ISO 179/1eA
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 178 °C ISO 11357-1/-3
Combustibilidad a 1.5mm esp. nom. HB class IEC 60695-11-10
Espesores de probeta 1.5 mm -
Yellow Card disponible - -
Combustibilidad a espesor h HB class IEC 60695-11-10
Espesores de probeta 0.8 mm -
Yellow Card disponible - -
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1400 kg/m³ ISO 1183
Funciones
Esfuerzo-alargamiento , Delrin® 100ALE NC010, POM-Z, DuPont
Módulo secante-alargamiento , Delrin® 100ALE NC010, POM-Z, DuPont
Características
Procesamiento y forma de entrega
Moldeo por inyección, Extrusión de perfiles, Extrusión de láminas, Otros tipos de extrusión
Forma de suministro
Sémola, Color natural
Aditivos
Lubricante, Desmoldeante
Características
Low Emission, Grado tribológico, Homopolímero
Applicaciones
Automotriz
Disponibilidad regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.