Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of AKROLEN® PP GFM 25/15 black (1415) - PP-(GF+MX)40 - Akro-Plastic GmbH

Material Data Center offers the following functions for AKROLEN® PP GFM 25/15 black (1415):
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Akrolen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 13.5 cm³/10min ISO 1133
Temperatura 230 °C -
Carga 2.16 kg -
Contracción posterior al moldeo, paralelo 0.5 % ISO 294-4, 2577
Contracción posterior al moldeo, normal 0.8 % ISO 294-4, 2577
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 6500 MPa ISO 527
Resistencia a la tracción 75 MPa ISO 527
Alargamiento a rotura 75 % ISO 527
Módulo de flexión, 23°C 6600 MPa ISO 178
Resistencia a la flexión 105 MPa ISO 178
Resistencia al impacto Charpy, +23°C 45 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C 45 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 10 kJ/m² ISO 179/1eA
Resistencia al impacto Izod con entalla, +23°C 10 kJ/m² ISO 180/1A
Ball indentation hardness 100 MPa ISO 2039-1
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 167 °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 150 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 163 °C ISO 75-1/-2
Coef.de expansión térmica lineal, paralelo 20 E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 125 E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. HB class IEC 60695-11-10
Espesores de probeta 1.6 mm -
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Resistividad volumétrica específica 2E9 Ohm*m IEC 62631-3-1
Resistencia dieléctrica 18 kV/mm IEC 60243-1
Indice comparativo de linea de fuga 600 - IEC 60112
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1210 kg/m³ ISO 1183
Funciones
Viscosidad-velocidad de cizallamiento , AKROLEN® PP GFM 25/15 black (1415), PP-(GF+MX)40, Akro-Plastic
Tensión de cizalla-velocidad de cizalla , AKROLEN® PP GFM 25/15 black (1415), PP-(GF+MX)40, Akro-Plastic
Volumen especifico-temperatura (pvT) , AKROLEN® PP GFM 25/15 black (1415), PP-(GF+MX)40, Akro-Plastic
Características
Forma de suministro
Negro
Características especiales
Estable contra el calor
Applicaciones
Automotriz, Electrica
Disponibilidad regional
Europa, Asia Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.